Recent changes

Jump to navigation Jump to search

Track the most recent changes to the wiki on this page.

Recent changes options Show last 50 | 100 | 250 | 500 changes in last 1 | 3 | 7 | 14 | 30 days
Hide registered users | Hide anonymous users | Hide my edits | Show bots | Hide minor edits
Show new changes starting from 17:34, 20 May 2024
   
List of abbreviations:
N
This edit created a new page (also see list of new pages)
m
This is a minor edit
b
This edit was performed by a bot
(±123)
The page size changed by this number of bytes

20 May 2024

     16:16  EDS‎‎ 2 changes history +824 [Bohnn‎ (2×)]
     
16:16 (cur | prev) +182 Bohnn talk contribs
     
13:55 (cur | prev) +642 Bohnn talk contribs →‎Overview
N    15:09  ALD-01: Aluminum Oxide Deposition‎‎ 10 changes history +464 [Lucasamb‎ (10×)]
     
15:09 (cur | prev) 0 Lucasamb talk contribs
     
15:06 (cur | prev) +1 Lucasamb talk contribs
     
15:05 (cur | prev) +14 Lucasamb talk contribs
     
14:58 (cur | prev) +1 Lucasamb talk contribs
     
14:58 (cur | prev) -1 Lucasamb talk contribs
     
14:58 (cur | prev) 0 Lucasamb talk contribs
     
14:58 (cur | prev) -1 Lucasamb talk contribs
     
14:57 (cur | prev) +1 Lucasamb talk contribs
     
14:57 (cur | prev) +221 Lucasamb talk contribs
N    
14:26 (cur | prev) +228 Lucasamb talk contribs Created page with "<iframe height="500px" key="google" level="docs" path="https://docs.google.com/spreadsheets/d/e/2PACX-1vRT0Xcfp3506lnri7h04_tPNBdXSckz1XCJizwMky8hWDH0QwxxVHefXI4scbtD66peP2nHN..."
N    14:45  SiO2 (silicon dioxide)‎‎ 12 changes history +2,184 [Dsabr‎ (12×)]
     
14:45 (cur | prev) +213 Dsabr talk contribs →‎Processes
     
14:44 (cur | prev) +89 Dsabr talk contribs →‎Processes
     
14:34 (cur | prev) +34 Dsabr talk contribs →‎ALD Master Recipe
     
14:33 (cur | prev) +551 Dsabr talk contribs →‎Processes
     
14:29 (cur | prev) +383 Dsabr talk contribs →‎Sputter Deposition Rates
     
14:25 (cur | prev) +68 Dsabr talk contribs →‎Etching Equipment
     
14:23 (cur | prev) +59 Dsabr talk contribs →‎Equipment
     
12:04 (cur | prev) +77 Dsabr talk contribs →‎Deposition Equipment
     
12:02 (cur | prev) +66 Dsabr talk contribs →‎Deposition Equipment
     
12:01 (cur | prev) +76 Dsabr talk contribs →‎Equipment
     
12:00 (cur | prev) -84 Dsabr talk contribs →‎Deposition Equipment
N    
12:00 (cur | prev) +652 Dsabr talk contribs Created page with "Silicon dioxide is an insulating, transparent oxide that is highly unreactive. It is often used as a passivation layer to protect electrical components. ==Equipment== ===..."
     14:42 Upload log Dsabr talk contribs uploaded File:Oxford PECVD SiO2 deposition.pdf
     14:11  Cambridge Nanotech S200 ALD diffhist +68 Lucasamb talk contribs →‎Applications
N    12:43  ToF-SIMS diffhist +593 Bohnn talk contribs Created page with "==Overview== '''Time of Flight Secondary Ion Mass Spectroscopy''' or '''ToF-SIMS''' is an technique performed in a FIB to analyze the composi..."
     10:53  Lesker PVD75 DC/RF Sputterer‎‎ 3 changes history +28 [Dsabr‎ (3×)]
     
10:53 (cur | prev) -11 Dsabr talk contribs →‎Oxides, fluorides & nitrides
     
10:52 (cur | prev) -1 Dsabr talk contribs →‎Oxides, fluorides & nitrides
     
10:52 (cur | prev) +40 Dsabr talk contribs →‎Oxides, fluorides & nitrides
     10:42  Denton Explorer14 Magnetron Sputterer‎‎ 2 changes history -10 [Dsabr‎ (2×)]
     
10:42 (cur | prev) -7 Dsabr talk contribs →‎Process data & master recipes
     
10:42 (cur | prev) -3 Dsabr talk contribs →‎Process data & master recipes

16 May 2024

     10:51  Denton Explorer14 Magnetron Sputterer diffhist +45 Dsabr talk contribs →‎SOPs & Troubleshooting
     10:50  (Upload log) [Dsabr‎ (2×)]
     
10:50 Dsabr talk contribs uploaded File:PVD 05 SOP.pdf
     
10:45 Dsabr talk contribs uploaded File:PVD 04 SOP.pdf
     10:46  Lesker PVD75 E-beam Evaporator diffhist +45 Dsabr talk contribs →‎SOPs & Troubleshooting
     10:42  Lesker PVD75 DC/RF Sputterer‎‎ 4 changes history +33 [Dsabr‎ (4×)]
     
10:42 (cur | prev) +48 Dsabr talk contribs →‎SOPs & troubleshooting
     
10:42 (cur | prev) -47 Dsabr talk contribs →‎Additional resources
     
10:41 (cur | prev) +14 Dsabr talk contribs →‎Metals
     
10:40 (cur | prev) +18 Dsabr talk contribs →‎Deposition sources

15 May 2024

N    14:24  ZEP Process Data diffhist +215 Dsbarth talk contribs Created page with "<iframe height="400px" key="google" level="docs" path="/spreadsheets/u/0/d/e/2PACX-1vSvZG1_8z70Dl9liA3fY2p8jojsyW4ELRhjOzFc7UKzOlXOxWQ4XkD6m_RAMx8-u2E5G21yPdKG6loM/pubchart?oi..."
     14:23  Raith EBPG5200+ E-Beam Lithography System‎‎ 2 changes history -22 [Dsbarth‎ (2×)]
     
14:23 (cur | prev) +48 Dsbarth talk contribs
     
09:18 (cur | prev) -70 Dsbarth talk contribs
     14:18  Lesker PVD75 DC/RF Sputterer‎‎ 3 changes history +49 [Dsabr‎ (3×)]
     
14:18 (cur | prev) 0 Dsabr talk contribs →‎Additional resources
     
14:17 (cur | prev) +13 Dsabr talk contribs →‎Additional resources
     
14:16 (cur | prev) +36 Dsabr talk contribs →‎Additional resources
     14:16  (User rights log) [Dsbarth‎ (4×)]
     
14:16 Dsbarth talk contribs changed group membership for Lucasamb from Editor to Editor and administrator ‎
     
14:16 Dsbarth talk contribs changed group membership for Coana from Editor to Editor and administrator ‎
     
14:16 Dsbarth talk contribs changed group membership for Dsabr from Editor to Editor and administrator ‎
     
14:15 Dsbarth talk contribs changed group membership for Azadi from Editor to Editor and administrator ‎
     14:16  Oxford PlasmaLab 100 PECVD‎‎ 2 changes history 0 [Azadi‎ (2×)]
     
14:16 (cur | prev) -66 Azadi talk contribs
     
14:15 (cur | prev) +66 Azadi talk contribs

10 May 2024

N    13:40  Keyence Profilometer diffhist +931 Bohnn talk contribs Created page with "Category:Characterization {{EquipmentInfo | name = Keyence Profilometer | Tool_Name = Keyence | image = 300px | imagecaption = | Instrument_Type = P..."
     13:37  (Upload log) [Bohnn‎ (2×)]
     
13:37 Bohnn talk contribs uploaded File:Keyence.jpg(image of keyence profilometer)
     
13:37 Bohnn talk contribs uploaded File:20240510 133218.jpg(image of keyence profilometer)
     11:39  SLPF Equipment diffhist +66 Bohnn talk contribs added keyence
     10:03  (Deletion log) [Dsbarth‎ (2×)]
     
10:03 Dsbarth talk contribs deleted page File:CharlesV.jpeg
     
10:01 Dsbarth talk contribs deleted page Charles Veith(content before blanking was: "__NOTOC__ {{StaffMemberInfobox |StaffName = Charles Veith |StaffPhoto = CharlesV.jpeg |JobTitle = Purchasing Manager <br> Vender Relations (NNCI) |AreasResponsibility = Purchasing <br> Micro Contamination |PennID = cveith |Phone = 508-579-5487 (office) |OfficeLocation = 110 Singh }} == About == ===== Role in the QNF ===== Charles R. Veith is a Member of Technical Staff in the Quattrone Nanofabrication Facility. His main responsibilities are owner and manager of...")
     10:00  QNF Staff diffhist -252 Dsbarth talk contribs

9 May 2024

 m   17:05  ABM3000HR Mask Aligner diffhist +17 Coana talk contribs reorganize information
     16:19  Lesker PVD75 DC/RF Sputterer‎‎ 6 changes history +32 [Dsabr‎ (6×)]
     
16:19 (cur | prev) +10 Dsabr talk contribs →‎DC deposition
     
14:09 (cur | prev) +9 Dsabr talk contribs →‎DC deposition
     
11:45 (cur | prev) +2 Dsabr talk contribs →‎DC deposition
     
11:44 (cur | prev) +11 Dsabr talk contribs →‎DC & RF sputtering process data
     
11:43 (cur | prev) -32 Dsabr talk contribs →‎SOPs & troubleshooting
     
10:10 (cur | prev) +32 Dsabr talk contribs →‎SOPs & troubleshooting
N    15:00  Au (gold)‎‎ 11 changes history +4,460 [Dsabr‎ (11×)]
     
15:00 (cur | prev) +7 Dsabr talk contribs →‎Sputter Deposition Rates
     
14:39 (cur | prev) -1 Dsabr talk contribs
     
14:39 (cur | prev) +138 Dsabr talk contribs →‎Processes
     
14:32 (cur | prev) -1 Dsabr talk contribs →‎Processes
     
14:31 (cur | prev) +88 Dsabr talk contribs →‎Processes
     
14:28 (cur | prev) +10 Dsabr talk contribs →‎Etching
     
14:21 (cur | prev) +182 Dsabr talk contribs
     
14:15 (cur | prev) +2,864 Dsabr talk contribs →‎Sputter Deposition Rates
     
14:11 (cur | prev) +1 Dsabr talk contribs →‎Sputter Deposition Rates
     
14:11 (cur | prev) +2 Dsabr talk contribs →‎Sputter Deposition Rates
N    
14:11 (cur | prev) +1,170 Dsabr talk contribs Created page with "==Equipment== ===Deposition Equipment=== * '''PVD-02:''' Lesker PVD75 E-Beam/Thermal Evaporator * '''PVD-03:''' Lesker PVD75..."
N    14:54  Ti (titanium)‎‎ 12 changes history +3,690 [Dsabr‎ (12×)]
     
14:54 (cur | prev) +196 Dsabr talk contribs →‎Processes
     
14:14 (cur | prev) +1 Dsabr talk contribs →‎Sputter Deposition Rates
     
14:14 (cur | prev) +2,090 Dsabr talk contribs →‎Sputter Deposition Rates
     
13:51 (cur | prev) +1 Dsabr talk contribs →‎Application
     
13:50 (cur | prev) 0 Dsabr talk contribs →‎Deposition Equipment
     
13:47 (cur | prev) -10 Dsabr talk contribs →‎Sputter Deposition Rates
     
13:42 (cur | prev) -8 Dsabr talk contribs →‎Sputter Deposition Rates
     
13:42 (cur | prev) -55 Dsabr talk contribs →‎Sputter Deposition Rates
     
13:42 (cur | prev) +256 Dsabr talk contribs →‎Sputter Deposition Rates
     
13:40 (cur | prev) +546 Dsabr talk contribs
     
11:59 (cur | prev) +34 Dsabr talk contribs
N    
11:56 (cur | prev) +639 Dsabr talk contribs Created page with "Titanium is a transition metal with atomic number 22 and symbol Ti. Titanium has a low density, high strength and is resistant to corrosion by water. It has relatively poor el..."
     10:09 Upload log Dsabr talk contribs uploaded File:PVD03 SOP v02.pdf
     09:52  Denton Explorer14 Magnetron Sputterer‎‎ 5 changes history 0 [Dsabr‎ (5×)]
     
09:52 (cur | prev) -173 Dsabr talk contribs →‎Master recipes
     
09:49 (cur | prev) +173 Dsabr talk contribs →‎Master recipes
     
09:42 (cur | prev) -173 Dsabr talk contribs →‎Master recipes
     
09:42 (cur | prev) -2 Dsabr talk contribs →‎Master recipes
     
09:41 (cur | prev) +175 Dsabr talk contribs →‎Master recipes

8 May 2024

 m   14:04  Raith EBPG5200+ E-Beam Lithography System diffhist +14 Dsbarth talk contribs

7 May 2024

     13:31  Raith EBPG5200+ E-Beam Lithography System‎‎ 2 changes history +47 [Dsbarth‎ (2×)]
     
13:31 (cur | prev) +12 Dsbarth talk contribs →‎Resources
     
13:19 (cur | prev) +35 Dsbarth talk contribs
     13:17 Upload log Dsbarth talk contribs uploaded File:EBPG5200+ SOP.pdf(SOP for EBL-03)