Difference between revisions of "Photolithography"
Jump to navigation
Jump to search
| Line 33: | Line 33: | ||
=====Internal Reports & Presentations===== | =====Internal Reports & Presentations===== | ||
| + | *[https://nemo.nano.upenn.edu/knowledge_base/user/items/categories/# Overview of Photolithography Capabilities at QNF] ''Singh Seminar Series, August 2025'' | ||
*[https://repository.upenn.edu/entities/publication/36e58b7d-2254-4e6b-b9b4-f1d247b98352 Effect of Developer Temperature on Photoresist Contrast in Grayscale Lithography] ''LW-01, SPR 220-3'' | *[https://repository.upenn.edu/entities/publication/36e58b7d-2254-4e6b-b9b4-f1d247b98352 Effect of Developer Temperature on Photoresist Contrast in Grayscale Lithography] ''LW-01, SPR 220-3'' | ||
*[https://repository.upenn.edu/entities/publication/2dc6357c-2974-47d6-b875-bfba1a5b59f5 Optimization of Bilayer Lift-Off Process to Enable the Gap Size of 1μm Using LOR 3A and S1813] | *[https://repository.upenn.edu/entities/publication/2dc6357c-2974-47d6-b875-bfba1a5b59f5 Optimization of Bilayer Lift-Off Process to Enable the Gap Size of 1μm Using LOR 3A and S1813] | ||
| − | *[https://repository.upenn.edu/entities/publication/86c27bd3-abdc-42cf-836a-671b350465fc Influence of flow rate, nozzle speed, pitch and the number of passes on the thickness of S1805 photoresist in SUSS MicroTec AS8 spray coater] ''RC-01 | + | *[https://repository.upenn.edu/entities/publication/86c27bd3-abdc-42cf-836a-671b350465fc Influence of flow rate, nozzle speed, pitch and the number of passes on the thickness of S1805 photoresist in SUSS MicroTec AS8 spray coater] ''RC-01'' |
*[https://repository.upenn.edu/entities/publication/f6608537-5d05-4c9f-8d9f-9bf9cc333b36 MicroChem S1818 Contrast Curve Optimization] ''MA-01'' | *[https://repository.upenn.edu/entities/publication/f6608537-5d05-4c9f-8d9f-9bf9cc333b36 MicroChem S1818 Contrast Curve Optimization] ''MA-01'' | ||
| − | *[https://repository.upenn.edu/entities/publication/c1f5aa27-e2be-4eb2-93ea-bf8a7efd35da Correction of pattern size deviations in the fabrication of photomasks made with a laser direct-writer] | + | *[https://repository.upenn.edu/entities/publication/c1f5aa27-e2be-4eb2-93ea-bf8a7efd35da Correction of pattern size deviations in the fabrication of photomasks made with a laser direct-writer] ''LW-01'' |
| − | *[https://repository.upenn.edu/entities/publication/1956d081-da9f-497f-b6f1-82f3d7c72196 Surface Treatment and Adhesion Study] | + | *[https://repository.upenn.edu/entities/publication/1956d081-da9f-497f-b6f1-82f3d7c72196 Surface Treatment and Adhesion Study] ''OVN-01'' |
| − | *[https://repository.upenn.edu/entities/publication/7ee1b740-1ff8-4ada-a5eb-81be1a090117 Heidelberg DWL66+ S1805 Contrast Curves] | + | *[https://repository.upenn.edu/entities/publication/7ee1b740-1ff8-4ada-a5eb-81be1a090117 Heidelberg DWL66+ S1805 Contrast Curves] ''LW-01'' |
| − | *[https://repository.upenn.edu/entities/publication/5bd0136f-e116-4721-9c84-164f17f04393 Heidelberg DWL66+ S1813 Contrast Curves] | + | *[https://repository.upenn.edu/entities/publication/5bd0136f-e116-4721-9c84-164f17f04393 Heidelberg DWL66+ S1813 Contrast Curves] ''LW-01'' |
*[https://repository.upenn.edu/entities/publication/1a9111e9-7e53-4e47-a11d-3fd34ce7de12 MicroChem S1800 Series Resist Application onto Si] | *[https://repository.upenn.edu/entities/publication/1a9111e9-7e53-4e47-a11d-3fd34ce7de12 MicroChem S1800 Series Resist Application onto Si] | ||
Revision as of 16:19, 29 August 2025
THIS PAGE IS UNDER CONSTRUCTION
About
Process Flow
QNF Example Protocols
Videos
Equipment at QNF
Patterning
- LW-01: Heidelberg DWL 66+ Laser Writer
- LW-02: Nanoscribe Photonic Professional GT
- LW-03: DMO MicroWriter ML3 Pro
- MA-01: SUSS MicroTec MA6 Gen3 Mask Aligner
- MA-03: ABM Mask Aligner
Resist Coating
- RC-01: SUSS MicroTec AS8 AltaSpray
- SPN-01: CEE Apogee Spinner - Acetone Soluble Photoresist
- SPN-03: CEE Apogee Spinner - LOR/PMGI
- SPN-06: CEE Apogee Spinner - E-Beam Resist
- SPN-08: CEE Apogee Spinner - Negative Epoxy
Additional Information
Related Wiki Pages
- How to Make a Mask
- Resists at QNF
- Developers at QNF -- Under Construction
- Ancillary Process Chemicals at QNF -- Under Construction
Internal Reports & Presentations
- Overview of Photolithography Capabilities at QNF Singh Seminar Series, August 2025
- Effect of Developer Temperature on Photoresist Contrast in Grayscale Lithography LW-01, SPR 220-3
- Optimization of Bilayer Lift-Off Process to Enable the Gap Size of 1μm Using LOR 3A and S1813
- Influence of flow rate, nozzle speed, pitch and the number of passes on the thickness of S1805 photoresist in SUSS MicroTec AS8 spray coater RC-01
- MicroChem S1818 Contrast Curve Optimization MA-01
- Correction of pattern size deviations in the fabrication of photomasks made with a laser direct-writer LW-01
- Surface Treatment and Adhesion Study OVN-01
- Heidelberg DWL66+ S1805 Contrast Curves LW-01
- Heidelberg DWL66+ S1813 Contrast Curves LW-01
- MicroChem S1800 Series Resist Application onto Si