*'''FABMATE Crucible:''' 99.9995% elemental carbon, internal volume: 4.4cc
 
*'''FABMATE Crucible:''' 99.9995% elemental carbon, internal volume: 4.4cc
 +
*'''Intermetallic Crucible:''' BN-TiB<sub>2</sub>, internal volume: 4.4cc
  
 
[[Image:Fabmate_4-4cc.png|500px]]
 
[[Image:Fabmate_4-4cc.png|500px]]

Latest revision as of 16:00, 1 October 2024

Jump to tool page

E-beam Crucible Liner Breakdown

  • FABMATE Crucible: 99.9995% elemental carbon, internal volume: 4.4cc
  • Intermetallic Crucible: BN-TiB2, internal volume: 4.4cc

Fabmate 4-4cc.png