User contributions
Jump to navigation
Jump to search
- 10:21, 13 January 2023 diff hist +105 SPTS Si DRIE →Description
- 10:16, 10 January 2023 diff hist +212 Oxford 80 Plus RIE →Description
- 15:24, 4 January 2023 diff hist +30 Cambridge Nanotech S200 ALD
- 15:23, 4 January 2023 diff hist +81 Cambridge Nanotech S200 ALD →Process Data
- 14:00, 16 December 2022 diff hist +117 Cambridge Nanotech S200 ALD
- 10:36, 15 December 2022 diff hist 0 Cambridge Nanotech S200 ALD
- 17:15, 14 December 2022 diff hist -1 Cambridge Nanotech S200 ALD
- 17:14, 14 December 2022 diff hist -9 Cambridge Nanotech S200 ALD
- 17:14, 14 December 2022 diff hist -5 Cambridge Nanotech S200 ALD
- 17:14, 14 December 2022 diff hist -10 Cambridge Nanotech S200 ALD
- 17:14, 14 December 2022 diff hist +53 Cambridge Nanotech S200 ALD
- 17:13, 14 December 2022 diff hist +90 Cambridge Nanotech S200 ALD →Process Data
- 10:56, 14 December 2022 diff hist +22 SPTS Si DRIE →Post etch sample cleaning procedure
- 17:42, 13 December 2022 diff hist +49 Sandvik Furnace Stack →Description
- 11:48, 9 December 2022 diff hist +10 SPTS Si DRIE →Sample cleaning procedure
- 11:47, 9 December 2022 diff hist +1 SPTS Si DRIE →Sample cleaning procedure
- 11:47, 9 December 2022 diff hist +290 SPTS Si DRIE →Description
- 10:53, 8 December 2022 diff hist 0 Cambridge Nanotech S200 ALD →Standard Processes
- 10:49, 8 December 2022 diff hist 0 Cambridge Nanotech S200 ALD
- 10:42, 8 December 2022 diff hist +3 Cambridge Nanotech S200 ALD
- 10:42, 8 December 2022 diff hist +577 Cambridge Nanotech S200 ALD
- 16:15, 6 December 2022 diff hist -6 Sandvik Furnace Stack →Applications
- 11:05, 6 December 2022 diff hist +2 Cambridge Nanotech S200 ALD
- 11:05, 6 December 2022 diff hist +19 Cambridge Nanotech S200 ALD
- 11:01, 6 December 2022 diff hist -20 Cambridge Nanotech S200 ALD →Deposition uniformity
- 11:01, 6 December 2022 diff hist +25 Cambridge Nanotech S200 ALD
- 10:59, 6 December 2022 diff hist +1 Cambridge Nanotech S200 ALD
- 10:59, 6 December 2022 diff hist +1 Cambridge Nanotech S200 ALD
- 10:58, 6 December 2022 diff hist -4 Cambridge Nanotech S200 ALD
- 10:58, 6 December 2022 diff hist +5 Cambridge Nanotech S200 ALD
- 10:58, 6 December 2022 diff hist +171 Cambridge Nanotech S200 ALD
- 10:56, 6 December 2022 diff hist 0 N File:600cyc .4 sec 8 sec dec 6 2022.png current
- 10:54, 6 December 2022 diff hist -3 Cambridge Nanotech S200 ALD
- 11:45, 29 November 2022 diff hist +1 Veeco Savannah 200
- 11:38, 29 November 2022 diff hist +1 Oxford PlasmaLab 100 PECVD
- 15:45, 28 November 2022 diff hist -1 Oxford PlasmaLab 100 PECVD →Deposition Rate Monitoring
- 15:44, 28 November 2022 diff hist +1 Oxford PlasmaLab 100 PECVD
- 15:44, 28 November 2022 diff hist -2 Oxford PlasmaLab 100 PECVD →Special process data - adjustable table temperature
- 15:44, 28 November 2022 diff hist -1 Oxford PlasmaLab 100 PECVD →Deposition Rate Monitoring
- 15:43, 28 November 2022 diff hist +94 Oxford PlasmaLab 100 PECVD
- 15:42, 28 November 2022 diff hist +41 Oxford PlasmaLab 100 PECVD
- 15:33, 28 November 2022 diff hist 0 N File:Sinx dep rate on cvd-01.jpg current
- 15:32, 28 November 2022 diff hist 0 N File:Sio2 dep on cvd-01.jpg current
- 11:33, 28 November 2022 diff hist +245 SUSS MicroTec AS8 AltaSpray →Resources
- 11:31, 28 November 2022 diff hist +147 Oxford 80 Plus RIE
- 10:53, 22 November 2022 diff hist +25 Jandel Multi Height Four Point Probe →SOPs & Troubleshooting
- 10:50, 22 November 2022 diff hist -1 SCS PDS2010 Parylene Coater →Resources
- 10:49, 22 November 2022 diff hist +171 SCS PDS2010 Parylene Coater →Resources
- 12:43, 18 November 2022 diff hist 0 Oxford PlasmaLab 100 PECVD →SOPs & Troubleshooting
- 11:03, 7 November 2022 diff hist +1 Oxford 80 Plus RIE →Etch Rate
- 11:02, 7 November 2022 diff hist +95 Oxford 80 Plus RIE →Etch Rate
- 10:04, 3 November 2022 diff hist -2 Oxford 80 Plus RIE
- 09:26, 3 November 2022 diff hist -3 Oxford 80 Plus RIE →Standard Process Information =
- 09:26, 3 November 2022 diff hist +39 Oxford 80 Plus RIE
- 16:25, 1 November 2022 diff hist +6 Oxford PlasmaLab 100 PECVD →Standard process data - Table temperature = 350 C
- 16:25, 1 November 2022 diff hist +2 Oxford PlasmaLab 100 PECVD →Resources
- 16:25, 1 November 2022 diff hist 0 Oxford PlasmaLab 100 PECVD →Special process data - adjustable table temperature
- 16:24, 1 November 2022 diff hist +281 Oxford PlasmaLab 100 PECVD
- 16:22, 1 November 2022 diff hist +143 Oxford PlasmaLab 100 PECVD
- 16:56, 31 October 2022 diff hist -1 Cambridge Nanotech S200 ALD
- 16:16, 31 October 2022 diff hist -6 Oxford PlasmaLab 100 PECVD
- 16:14, 31 October 2022 diff hist +522 Oxford PlasmaLab 100 PECVD
- 12:13, 28 October 2022 diff hist +109 Cambridge Nanotech S200 ALD →Standard Processes
- 09:26, 28 October 2022 diff hist +9 Cambridge Nanotech S200 ALD
- 09:36, 26 October 2022 diff hist +1 Cambridge Nanotech S200 ALD
- 09:36, 26 October 2022 diff hist +37 Cambridge Nanotech S200 ALD
- 09:28, 26 October 2022 diff hist +40 Cambridge Nanotech S200 ALD
- 09:28, 26 October 2022 diff hist 0 N File:Alumina Oct6.jpg current
- 09:26, 26 October 2022 diff hist +39 Cambridge Nanotech S200 ALD
- 09:22, 26 October 2022 diff hist 0 N File:Hafnia Oct6.jpg current
- 16:41, 19 October 2022 diff hist +39 N File:HfO2.png HfO2 process control 150C current
- 16:37, 19 October 2022 diff hist +46 N File:Alumina.png ALD alumina process control_150C current
- 16:08, 18 October 2022 diff hist +1 Veeco Savannah 200
- 16:07, 18 October 2022 diff hist +47 Veeco Savannah 200 →Most Recent Deposition Rates
- 16:07, 18 October 2022 diff hist +60 Veeco Savannah 200 →Most Recent Deposition Rates
- 15:28, 18 October 2022 diff hist +8 Veeco Savannah 200
- 15:10, 18 October 2022 diff hist +105 Veeco Savannah 200
- 15:04, 18 October 2022 diff hist +589 Veeco Savannah 200
- 16:03, 3 October 2022 diff hist +132 Sandvik Furnace Stack
- 16:01, 3 October 2022 diff hist +205 Sandvik Furnace Stack
- 15:51, 3 October 2022 diff hist +375 Oxford 80 Plus RIE
- 15:39, 3 October 2022 diff hist +33 Oxford PlasmaLab 100 PECVD
- 15:27, 3 October 2022 diff hist +501 Oxford PlasmaLab 100 PECVD
- 13:05, 27 September 2022 diff hist +1 Cambridge Nanotech S200 ALD
- 11:55, 27 September 2022 diff hist +1 Cambridge Nanotech S200 ALD
- 11:18, 27 September 2022 diff hist +510 Cambridge Nanotech S200 ALD
- 10:04, 27 September 2022 diff hist -23 Cambridge Nanotech S200 ALD
- 10:03, 27 September 2022 diff hist +211 Cambridge Nanotech S200 ALD
- 12:37, 19 September 2022 diff hist -640 Sandvik Furnace Stack
- 09:27, 2 September 2022 diff hist +105 Process Resources
- 17:00, 1 September 2022 diff hist +111 Process Resources
- 16:44, 1 September 2022 diff hist +26 Process Resources
- 10:14, 18 May 2022 diff hist -4 Oxford Cobra ICP Etcher →Resources
- 10:14, 18 May 2022 diff hist +82 Oxford Cobra ICP Etcher →Resources
- 16:51, 5 May 2022 diff hist 0 Denton Explorer14 Magnetron Sputterer →Deposition Power
- 16:51, 5 May 2022 diff hist +7 Denton Explorer14 Magnetron Sputterer
- 16:50, 5 May 2022 diff hist +72 Denton Explorer14 Magnetron Sputterer →Deposition Power
- 16:49, 5 May 2022 diff hist +489 Denton Explorer14 Magnetron Sputterer →Deposition Power
- 16:42, 5 May 2022 diff hist -3 Denton Explorer14 Magnetron Sputterer →Deposition Power
- 16:42, 5 May 2022 diff hist -41 Denton Explorer14 Magnetron Sputterer →Deposition Power