Difference between revisions of "Resists at QNF"
Jump to navigation
Jump to search
(→Stockroom Photoresists: Remover set to N/A) |
(Including thickness) |
||
Line 7: | Line 7: | ||
| [https://amolf.nl/wp-content/uploads/2016/09/datasheets_S1800.pdf S1805] || + || PGMEA || General || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], [https://wiki.nano.upenn.edu/wiki/index.php?title=Heidelberg_DWL_66%2B_Laser_Writer LW-01], SPN-03 || MF-319 (0.24N TMAH) || MP 1165 (NMP) || KL5305 | | [https://amolf.nl/wp-content/uploads/2016/09/datasheets_S1800.pdf S1805] || + || PGMEA || General || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], [https://wiki.nano.upenn.edu/wiki/index.php?title=Heidelberg_DWL_66%2B_Laser_Writer LW-01], SPN-03 || MF-319 (0.24N TMAH) || MP 1165 (NMP) || KL5305 | ||
|- | |- | ||
− | | [https://amolf.nl/wp-content/uploads/2016/09/datasheets_S1800.pdf S1813] || + || PGMEA || General || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], [https://wiki.nano.upenn.edu/wiki/index.php?title=Heidelberg_DWL_66%2B_Laser_Writer LW-01], SPN-03 || MF-319 (0.24N TMAH) || MP 1165 (NMP) || KL5315 | + | | [https://amolf.nl/wp-content/uploads/2016/09/datasheets_S1800.pdf S1813] || + || PGMEA || General, 1um-1.3um || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], [https://wiki.nano.upenn.edu/wiki/index.php?title=Heidelberg_DWL_66%2B_Laser_Writer LW-01], SPN-03 || MF-319 (0.24N TMAH) || MP 1165 (NMP) || KL5315 |
|- | |- | ||
| [https://amolf.nl/wp-content/uploads/2016/09/datasheets_S1800.pdf S1818] || + || PGMEA || General || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], [https://wiki.nano.upenn.edu/wiki/index.php?title=Heidelberg_DWL_66%2B_Laser_Writer LW-01], SPN-03 || MF-319 (0.24N TMAH) || MP 1165 (NMP) || | | [https://amolf.nl/wp-content/uploads/2016/09/datasheets_S1800.pdf S1818] || + || PGMEA || General || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], [https://wiki.nano.upenn.edu/wiki/index.php?title=Heidelberg_DWL_66%2B_Laser_Writer LW-01], SPN-03 || MF-319 (0.24N TMAH) || MP 1165 (NMP) || | ||
|- | |- | ||
− | | [https://upenn.box.com/s/lpd3ev35603w582la2317tkubb36ylzt SPR 220-3] || + || Ethyl lactate, anisole, n-amyl acetate || Etch || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || 0.24N TMAH || MP 1165 (NMP) || KPRO-3, KL6003, AZ3330F | + | | [https://upenn.box.com/s/lpd3ev35603w582la2317tkubb36ylzt SPR 220-3] || + || Ethyl lactate, anisole, n-amyl acetate || Etch, 2um-5um || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || 0.24N TMAH || MP 1165 (NMP) || KPRO-3, KL6003, AZ3330F |
|- | |- | ||
| [https://upenn.box.com/s/lpd3ev35603w582la2317tkubb36ylzt SPR 220-4.5] || + || Ethyl lactate, anisole, n-amyl acetate || Etch || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || 0.24N TMAH || MP 1165 (NMP) || KPRO-3, KL6003, AZ3330F | | [https://upenn.box.com/s/lpd3ev35603w582la2317tkubb36ylzt SPR 220-4.5] || + || Ethyl lactate, anisole, n-amyl acetate || Etch || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || 0.24N TMAH || MP 1165 (NMP) || KPRO-3, KL6003, AZ3330F | ||
|- | |- | ||
− | | [https://upenn.box.com/s/lpd3ev35603w582la2317tkubb36ylzt SPR 220-7] || + || Ethyl lactate, anisole, n-amyl acetate || Etch || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || 0.24N TMAH or 0.26N TMAH || MP 1165 (NMP) || AZ 12XT, AZ P4620 | + | | [https://upenn.box.com/s/lpd3ev35603w582la2317tkubb36ylzt SPR 220-7] || + || Ethyl lactate, anisole, n-amyl acetate || Etch, 6um-12um || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || 0.24N TMAH or 0.26N TMAH || MP 1165 (NMP) || AZ 12XT, AZ P4620 |
|- | |- | ||
| [https://upenn.box.com/s/xb5pfl6zbb1eynl6oyerrub0lw3xh3n7 AZ 3330F] || + || PGMEA || General, Metal RIE, Plating || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || AZ300 (0.26N TMAH) or AZ400K 1:4 (potassium salts) || || SPR 220-3, SPR 220-4.5, K-PRO 3, KL6003 | | [https://upenn.box.com/s/xb5pfl6zbb1eynl6oyerrub0lw3xh3n7 AZ 3330F] || + || PGMEA || General, Metal RIE, Plating || [https://wiki.nano.upenn.edu/wiki/index.php?title=SUSS_MicroTec_MA6_Gen3_Mask_Aligner MA-01], SPN-03 || AZ300 (0.26N TMAH) or AZ400K 1:4 (potassium salts) || || SPR 220-3, SPR 220-4.5, K-PRO 3, KL6003 | ||
Line 34: | Line 34: | ||
! Name / Datasheet !! Tone !! Composition !! Use / Thickness !! Tool Compatibility !! Developer !! Remover !! Alternative Resists | ! Name / Datasheet !! Tone !! Composition !! Use / Thickness !! Tool Compatibility !! Developer !! Remover !! Alternative Resists | ||
|- | |- | ||
− | | [https://upenn.box.com/s/f9oi75p3p84rdtpqq5unp0j1c3mqxjrd SU-8 2005] || - || Cyclopentanone || Epoxy || [https://wiki.nano.upenn.edu/wiki/index.php?title=Spinner_-_SU-8/PDMS SPN-07], [https://wiki.nano.upenn.edu/wiki/index.php?title=ABM3000HR_Mask_Aligner MA-03] || SU-8 Developer (PGMEA) || N/A || HARE SQ 2 | + | | [https://upenn.box.com/s/f9oi75p3p84rdtpqq5unp0j1c3mqxjrd SU-8 2005] || - || Cyclopentanone || Epoxy, 4um-7um || [https://wiki.nano.upenn.edu/wiki/index.php?title=Spinner_-_SU-8/PDMS SPN-07], [https://wiki.nano.upenn.edu/wiki/index.php?title=ABM3000HR_Mask_Aligner MA-03] || SU-8 Developer (PGMEA) || N/A || HARE SQ 2 |
|- | |- | ||
− | | [https://upenn.box.com/s/s4noknbqlyh8inq3gqycw115b7ufdibu SU-8 2050] || - || Cyclopentanone || Epoxy || [https://wiki.nano.upenn.edu/wiki/index.php?title=Spinner_-_SU-8/PDMS SPN-07], [https://wiki.nano.upenn.edu/wiki/index.php?title=ABM3000HR_Mask_Aligner MA-03] || SU-8 Developer (PGMEA) || N/A || HARE SQ 50 | + | | [https://upenn.box.com/s/s4noknbqlyh8inq3gqycw115b7ufdibu SU-8 2050] || - || Cyclopentanone || Epoxy, 40um-170um || [https://wiki.nano.upenn.edu/wiki/index.php?title=Spinner_-_SU-8/PDMS SPN-07], [https://wiki.nano.upenn.edu/wiki/index.php?title=ABM3000HR_Mask_Aligner MA-03] || SU-8 Developer (PGMEA) || N/A || HARE SQ 50 |
|- | |- | ||
| [https://upenn.box.com/s/va40gxhk7ghwl8p9hhsyvr0rairc9v1e SU-8 2100] || - || Cyclopentanone || Epoxy || [https://wiki.nano.upenn.edu/wiki/index.php?title=Spinner_-_SU-8/PDMS SPN-07], [https://wiki.nano.upenn.edu/wiki/index.php?title=ABM3000HR_Mask_Aligner MA-03] || SU-8 Developer (PGMEA) || N/A || HARE SQ 50 | | [https://upenn.box.com/s/va40gxhk7ghwl8p9hhsyvr0rairc9v1e SU-8 2100] || - || Cyclopentanone || Epoxy || [https://wiki.nano.upenn.edu/wiki/index.php?title=Spinner_-_SU-8/PDMS SPN-07], [https://wiki.nano.upenn.edu/wiki/index.php?title=ABM3000HR_Mask_Aligner MA-03] || SU-8 Developer (PGMEA) || N/A || HARE SQ 50 | ||
Line 49: | Line 49: | ||
| [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 495 PMMA A8] || + || Anisole || Lower Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 495 PMMA A8] || + || Anisole || Lower Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || | ||
|- | |- | ||
− | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 495 PMMA A4] || + || Anisole || Lower Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || | + | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 495 PMMA A4] || + || Anisole || Lower Resolution, 180nm-300nm || [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || |
|- | |- | ||
− | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 495 PMMA A2] || + || Anisole || Lower Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || | + | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 495 PMMA A2] || + || Anisole || Lower Resolution, 50nm-100nm || [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || |
|- | |- | ||
− | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 950 PMMA A4] || + || Anisole || High Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || | + | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 950 PMMA A4] || + || Anisole || High Resolution, 200nm-400nm || [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || |
|- | |- | ||
− | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 950 PMMA A2] || + || Anisole || High Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || 1000 HARP 0.1 | + | | [https://upenn.box.com/s/ff9s9dhl52tqagc0vbtflwf64odcwtw7 950 PMMA A2] || + || Anisole || High Resolution, 50nm-100nm || [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || 1000 HARP 0.1 |
|- | |- | ||
| [https://upenn.box.com/s/re1sz5cil83m99yv3ug2p9p8ghk3a3vm 1000 HARP 1.3] || + || Anisole || High Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || | | [https://upenn.box.com/s/re1sz5cil83m99yv3ug2p9p8ghk3a3vm 1000 HARP 1.3] || + || Anisole || High Resolution|| [https://wiki.nano.upenn.edu/wiki/index.php?title=Elionix_ELS-7500EX_E-Beam_Lithography_System EBL-01], SPN-06 || MIBK || NMP || | ||
Line 100: | Line 100: | ||
| [https://upenn.box.com/s/v0hwe0p0u3la1oodz3g45qjw0yl54z7f K-PRO 3] || + || PGMEA || Plating, Etching || || 0.26N TMAH or alkaline salts || NMP, DMSO || SPR 220-3, SPR 220-4.5 | | [https://upenn.box.com/s/v0hwe0p0u3la1oodz3g45qjw0yl54z7f K-PRO 3] || + || PGMEA || Plating, Etching || || 0.26N TMAH or alkaline salts || NMP, DMSO || SPR 220-3, SPR 220-4.5 | ||
|- | |- | ||
− | | [https://upenn.box.com/s/dj5l9rrsg0k8g8opdegrylhkgypev9w9 AZ 12XT-20PL-15] || + || PGMEA || CAR (i-line), Plating, Packaging, Deep Etch || || AZ300 (0.26N TMAH) || || SPR 220-7, AZ P4620 | + | | [https://upenn.box.com/s/dj5l9rrsg0k8g8opdegrylhkgypev9w9 AZ 12XT-20PL-15] || + || PGMEA || CAR (i-line), Plating, Packaging, Deep Etch, 10um-25um || || AZ300 (0.26N TMAH) || || SPR 220-7, AZ P4620 |
|- | |- | ||
| [https://upenn.box.com/s/0r8meepoyq0b1jux7ubudcpt70clau48 AZ P4620] || + || PGMEA || Thick Resist, Plating, Packaging || || AZ300 (0.26N TMAH) or AZ400K 1:4 (potassium salts) || || SPR 220-7, AZ 12XT-20PL-15 | | [https://upenn.box.com/s/0r8meepoyq0b1jux7ubudcpt70clau48 AZ P4620] || + || PGMEA || Thick Resist, Plating, Packaging || || AZ300 (0.26N TMAH) or AZ400K 1:4 (potassium salts) || || SPR 220-7, AZ 12XT-20PL-15 |
Revision as of 16:58, 30 June 2023
The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Click on the resist name to access the datasheet. Other similar options that may be available in QNF are also listed.
QNF Supplied Standard Photoresists
Name / Datasheet | Tone | Composition | Use / Thickness | Tool Compatibility | Developer | Remover | Alternative Resists |
---|---|---|---|---|---|---|---|
S1805 | + | PGMEA | General | MA-01, LW-01, SPN-03 | MF-319 (0.24N TMAH) | MP 1165 (NMP) | KL5305 |
S1813 | + | PGMEA | General, 1um-1.3um | MA-01, LW-01, SPN-03 | MF-319 (0.24N TMAH) | MP 1165 (NMP) | KL5315 |
S1818 | + | PGMEA | General | MA-01, LW-01, SPN-03 | MF-319 (0.24N TMAH) | MP 1165 (NMP) | |
SPR 220-3 | + | Ethyl lactate, anisole, n-amyl acetate | Etch, 2um-5um | MA-01, SPN-03 | 0.24N TMAH | MP 1165 (NMP) | KPRO-3, KL6003, AZ3330F |
SPR 220-4.5 | + | Ethyl lactate, anisole, n-amyl acetate | Etch | MA-01, SPN-03 | 0.24N TMAH | MP 1165 (NMP) | KPRO-3, KL6003, AZ3330F |
SPR 220-7 | + | Ethyl lactate, anisole, n-amyl acetate | Etch, 6um-12um | MA-01, SPN-03 | 0.24N TMAH or 0.26N TMAH | MP 1165 (NMP) | AZ 12XT, AZ P4620 |
AZ 3330F | + | PGMEA | General, Metal RIE, Plating | MA-01, SPN-03 | AZ300 (0.26N TMAH) or AZ400K 1:4 (potassium salts) | SPR 220-3, SPR 220-4.5, K-PRO 3, KL6003 | |
NR7-3000P | - | Cyclohexanone | Etch, General | MA-01 | RD6 (0.24N or 0.26N TMAH) | RR4 (DMSO), Acetone | |
APOL-LO 3202 | - | PGMEA | Liftoff | MA-01 | 0.26N TMAH | NMP, DMSO | |
IP-Dip | - | Ethoxylated acrylates | Nanoscribe, Epoxy | LW-02 | PGMEA, IPA | ||
HARE SQ 2 | - | Cyclopentanone, gamma butyro lactone | Epoxy | SPN-07, MA-03 | PGMEA | N/A | SU-8 2005 |
HARE SQ 50 | - | Cyclopentanone, gamma butyro lactone | Epoxy | SPN-07, MA-03 | PGMEA | N/A | SU-8 2050 |
Stockroom Photoresists
Name / Datasheet | Tone | Composition | Use / Thickness | Tool Compatibility | Developer | Remover | Alternative Resists |
---|---|---|---|---|---|---|---|
SU-8 2005 | - | Cyclopentanone | Epoxy, 4um-7um | SPN-07, MA-03 | SU-8 Developer (PGMEA) | N/A | HARE SQ 2 |
SU-8 2050 | - | Cyclopentanone | Epoxy, 40um-170um | SPN-07, MA-03 | SU-8 Developer (PGMEA) | N/A | HARE SQ 50 |
SU-8 2100 | - | Cyclopentanone | Epoxy | SPN-07, MA-03 | SU-8 Developer (PGMEA) | N/A | HARE SQ 50 |
SU-8 3050 | - | Cyclopentanone | Epoxy | SPN-07, MA-03 | SU-8 Developer (PGMEA) | N/A | HARE SQ 50 |
Standard e-beam Resists
Name / Datasheet | Tone | Composition | Use / Thickness | Tool Compatibility | Developer | Remover | Alternative Resists |
---|---|---|---|---|---|---|---|
495 PMMA A8 | + | Anisole | Lower Resolution | EBL-01, SPN-06 | MIBK | NMP | |
495 PMMA A4 | + | Anisole | Lower Resolution, 180nm-300nm | EBL-01, SPN-06 | MIBK | NMP | |
495 PMMA A2 | + | Anisole | Lower Resolution, 50nm-100nm | EBL-01, SPN-06 | MIBK | NMP | |
950 PMMA A4 | + | Anisole | High Resolution, 200nm-400nm | EBL-01, SPN-06 | MIBK | NMP | |
950 PMMA A2 | + | Anisole | High Resolution, 50nm-100nm | EBL-01, SPN-06 | MIBK | NMP | 1000 HARP 0.1 |
1000 HARP 1.3 | + | Anisole | High Resolution | EBL-01, SPN-06 | MIBK | NMP | |
1000 HARP 0.1 | + | Anisole | High Resolution | EBL-01, SPN-06 | MIBK | NMP | 950 PMMA A2 |
Stockroom e-beam Resists
Name / Datasheet | Tone | Composition | Use / Thickness | Tool Compatibility | Developer | Remover |
---|---|---|---|---|---|---|
ZEP 520A | + | Anisole | Thicker formulation | EBL-01, SPN-06 | Xylenes, n-amyl acetate or MIBK | NMP |
ZEP 520A-7 | + | Anisole | Thinner formulation | EBL-01, SPN-06 | Xylenes, n-amyl acetate or MIBK | NMP |
H-SiQ 6% | - | MIBK | HSQ Equivalent | EBL-01, SPN-06 | TMAH |
Other Resists
Name / Datasheet | Tone | Composition | Use / Thickness | Tool Compatibility | Developer | Remover |
---|---|---|---|---|---|---|
LOR 3A | N/A | Cyclopentanone, PGME | Liftoff, Non-imaging | Keep away from acetone & PGMEA | 0.24N TMAH, 0.26N TMAH | 1165 or Remover PG (NMP) |
PMGI SF 5S | N/A | Cyclopentanone, PGME | Liftoff, Non-imaging | Keep away from acetone & PGMEA | 0.24N TMAH, 0.26N TMAH | 1165 or Remover PG (NMP) |
PMGI SF 2S | N/A | Cyclopentanone, PGME | Liftoff, Non-imaging | Keep away from acetone & PGMEA | 0.24N TMAH, 0.26N TMAH | 1165 or Remover PG (NMP) |
NXR-1025 | N/A | Stockroom, Nanoimprint | MA-02 |
Miscellaneous
These may be available but are not guaranteed to be stocked
Name / Datasheet | Tone | Composition | Use / Thickness | Tool Compatibility | Developer | Remover | Alternative Resists |
---|---|---|---|---|---|---|---|
KL5305 | + | PGMEA | General | 0.26N TMAH | NMP, DMSO | S1805 | |
KL5315 | + | PGMEA | General | 0.26N TMAH | NMP, DMSO | S1813 | |
KL6003 | + | PGMEA | 0.26N TMAH | NMP, DMSO | SPR 220-3, SPR 220-4.5 | ||
K-PRO 3 | + | PGMEA | Plating, Etching | 0.26N TMAH or alkaline salts | NMP, DMSO | SPR 220-3, SPR 220-4.5 | |
AZ 12XT-20PL-15 | + | PGMEA | CAR (i-line), Plating, Packaging, Deep Etch, 10um-25um | AZ300 (0.26N TMAH) | SPR 220-7, AZ P4620 | ||
AZ P4620 | + | PGMEA | Thick Resist, Plating, Packaging | AZ300 (0.26N TMAH) or AZ400K 1:4 (potassium salts) | SPR 220-7, AZ 12XT-20PL-15 | ||
ma-N 2403 | - | e-beam/DUV Mix and Match |