The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool.  The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd via e-beam evaporation. The tool also comes with a load-lock system, allowing for fast and easy transfer of samples in and out of the system.
+
The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool.  The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd. The tool also comes with a load-lock, allowing for fast and easy transfer of samples in and out of the system. While less flexible than the [[Lesker PVD75 E-Beam/Thermal Evaporator | PVD-02]] deposition system in terms of available materials, the PVD-04 is a much faster tool.
  
 
===== Available materials =====
 
===== Available materials =====

Revision as of 08:46, 14 September 2022


Lesker PVD75 E-Beam/Thermal Evaporator
PVD-04.jpeg
Tool Name Lesker PVD75 E-Beam/Thermal Evaporator
Instrument Type Physical vapor deposition
Staff Manager Jason (jarohr@seas.upenn.edu)
Lab Location Bay 2
Tool Manufacturer Kurt J. Lesker
Tool Model PVD75
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone 8-9748
SOP Link SOP

Description

The tool

The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool. The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd. The tool also comes with a load-lock, allowing for fast and easy transfer of samples in and out of the system. While less flexible than the PVD-02 deposition system in terms of available materials, the PVD-04 is a much faster tool.

Available materials

The tool contains the following materials:

  • Au - Gold
  • Cr - Chromium
  • Pd - Palladium
  • Ti - Titanium

Deposition is limited to thin-film thicknesses of ~100 nm.