- 15:23, 27 September 2023 diff hist +52 Lesker PVD75 DC/RF Sputterer →DC deposition
- 10:08, 18 August 2023 diff hist -45 Denton Explorer14 Magnetron Sputterer →Process data & master recipes
- 10:08, 18 August 2023 diff hist +13 Denton Explorer14 Magnetron Sputterer →Process data & master recipes
- 10:07, 18 August 2023 diff hist 0 Denton Explorer14 Magnetron Sputterer →Process data & master recipes
- 16:50, 27 June 2023 diff hist +11 Lesker PVD75 DC/RF Sputterer →DC deposition
- 10:52, 25 April 2023 diff hist +2 Denton Explorer14 Magnetron Sputterer →Process data & master recipes
- 10:51, 25 April 2023 diff hist +30 Denton Explorer14 Magnetron Sputterer →Process data & master recipes
- 10:24, 5 April 2023 diff hist +39 Lesker PVD75 DC/RF Sputterer →DC deposition
- 13:49, 7 March 2023 diff hist +97 Lesker PVD75 DC/RF Sputterer →Deposition sources
- 13:46, 7 March 2023 diff hist +28 Denton Explorer14 Magnetron Sputterer →Process data & master recipes
- 17:46, 6 March 2023 diff hist +37 Lesker PVD75 DC/RF Sputterer →DC deposition
- 17:45, 6 March 2023 diff hist +40 Lesker PVD75 DC/RF Sputterer →DC deposition
- 17:43, 6 March 2023 diff hist +37 Lesker PVD75 DC/RF Sputterer →DC deposition
- 13:13, 27 February 2023 diff hist +39 Lesker PVD75 DC/RF Sputterer →RF deposition
- 13:12, 27 February 2023 diff hist +34 Lesker PVD75 DC/RF Sputterer →DC & RF sputtering process data
- 16:52, 2 February 2023 diff hist +38 Lesker PVD75 DC/RF Sputterer →DC deposition
- 13:39, 31 January 2023 diff hist -10 W master recipe current
- 12:35, 31 January 2023 diff hist +705 W master recipe
- 12:32, 31 January 2023 diff hist +801 Pt master recipe current
- 12:31, 31 January 2023 diff hist +35 Au master recipe current
- 12:30, 31 January 2023 diff hist +743 Au master recipe
- 12:27, 31 January 2023 diff hist +876 Ag master recipe current
- 15:03, 30 January 2023 diff hist +30 W master recipe
- 15:03, 30 January 2023 diff hist +30 Ti master recipe current
- 15:02, 30 January 2023 diff hist +30 Pt master recipe
- 15:02, 30 January 2023 diff hist +30 Mo master recipe current
- 15:02, 30 January 2023 diff hist +30 Cu master recipe current
- 15:02, 30 January 2023 diff hist +30 Au master recipe
- 15:02, 30 January 2023 diff hist +30 Al master recipe current
- 15:01, 30 January 2023 diff hist +30 Ag master recipe
- 15:00, 30 January 2023 diff hist +18 W master recipe
- 15:00, 30 January 2023 diff hist +18 Ti master recipe
- 14:59, 30 January 2023 diff hist -9 Pt master recipe
- 14:59, 30 January 2023 diff hist -11 Mo master recipe
- 14:59, 30 January 2023 diff hist +2,063 Mo master recipe
- 14:59, 30 January 2023 diff hist -2,063 Denton Explorer14 Magnetron Sputterer →Molybdenum (Mo)
- 14:58, 30 January 2023 diff hist +18 Cu master recipe
- 14:58, 30 January 2023 diff hist +18 Au master recipe
- 14:58, 30 January 2023 diff hist +18 Al master recipe
- 14:58, 30 January 2023 diff hist -2 Ag master recipe
- 14:58, 30 January 2023 diff hist +6 Ag master recipe
- 14:57, 30 January 2023 diff hist +6 Ag master recipe
- 14:57, 30 January 2023 diff hist +8 Ag master recipe
- 14:56, 30 January 2023 diff hist +37 W master recipe
- 14:56, 30 January 2023 diff hist +2,058 N W master recipe W master recipe
- 14:55, 30 January 2023 diff hist +22 Denton Explorer14 Magnetron Sputterer →Process data & master recipes
- 14:55, 30 January 2023 diff hist -2,060 Denton Explorer14 Magnetron Sputterer →Tungsten (W)
- 14:55, 30 January 2023 diff hist +2,061 Pt master recipe
- 14:54, 30 January 2023 diff hist -2,061 Denton Explorer14 Magnetron Sputterer →Platinum (Pt)
- 14:54, 30 January 2023 diff hist +2,057 Au master recipe