Difference between revisions of "Lesker PVD75 E-beam Evaporator"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(update tool owner)
(update to NEMO)
Line 11: Line 11:
 
| Tool_Manufacturer = Kurt J. Lesker
 
| Tool_Manufacturer = Kurt J. Lesker
 
| Tool_Model = PVD75
 
| Tool_Model = PVD75
| Iris_Designation = PVD-04
+
| NEMO_Designation = PVD-04
 
| Lab_Phone = 215-898-9748
 
| Lab_Phone = 215-898-9748
 
| SOP Link = [https://www.seas.upenn.edu/~nanosop/PVD75_e-beam_SOP.htm SOP]
 
| SOP Link = [https://www.seas.upenn.edu/~nanosop/PVD75_e-beam_SOP.htm SOP]

Revision as of 12:54, 3 January 2024


Lesker PVD75 E-Beam/Thermal Evaporator
PVD-04.jpeg
Tool Name Lesker PVD75 E-Beam/Thermal Evaporator
Instrument Type Physical vapor deposition
Staff Manager David Barth
Lab Location Bay 2
Tool Manufacturer Kurt J. Lesker
Tool Model PVD75
NEMO Designation PVD-04
Nearest Phone 215-898-9748
SOP Link SOP

Description

The tool

The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool. The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd. The tool also comes with a load-lock, allowing for fast and easy transfer of samples in and out of the system. While less flexible than the PVD-02 deposition system in terms of available materials, the PVD-04 is a much faster tool.

Available materials

The tool contains the following materials:

  • Au - Gold
  • Cr - Chromium
  • Pd - Palladium
  • Ti - Titanium

Deposition is limited to thin-film thicknesses of ~100 nm.