Tousimis Critical Point Dryer
Jump to navigation
Jump to search
![]() |
|
Tool Name | Tousimis Critical Point Dryer |
---|---|
Instrument Type | Back End |
Staff Manager | Kyle Keenan |
Lab Location | Bay 3 |
Tool Manufacturer | Tousimis |
Tool Model | 931-C |
NEMO Designation | CPD-01 |
Nearest Phone | XXXXX |
SOP Link | SOP |
Description
The system enables drying of delicate samples through the use of liquid carbon dioxide as a transitional fluid which has zero surface tension at the critical point (1072 psi at 31 C). The tool can process pieces up to several 100 mm substrates.
Applications
- Carbon dioxide (CO2) drying after release of bulk or surface micromachined devices