Difference between revisions of "Oxford Cobra ICP Etcher"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
m
(update to NEMO)
Line 11: Line 11:
 
| Tool_Manufacturer = Oxford Instruments
 
| Tool_Manufacturer = Oxford Instruments
 
| Tool_Model = Cobra PlasmaPro 100
 
| Tool_Model = Cobra PlasmaPro 100
| Iris_Designation = DE-05
+
| NEMO_Designation = DE-05
 
| Lab_Phone = 215-898-9748
 
| Lab_Phone = 215-898-9748
 
| SOP Link = [https://repository.upenn.edu/scn_sop/19/ SOP]
 
| SOP Link = [https://repository.upenn.edu/scn_sop/19/ SOP]

Revision as of 13:08, 3 January 2024


Oxford Cobra ICP Etcher
DE-05.jpeg
Tool Name Oxford Cobra ICP Etcher
Instrument Type Etch
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer Oxford Instruments
Tool Model Cobra PlasmaPro 100
NEMO Designation DE-05
Nearest Phone 215-898-9748
SOP Link SOP

Description

Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures.

  • Max ICP power: 3 kW
  • Max RF power: 200 W

The tool is connected to the following gases: BCl3, Cl2, Ar, O2, SF6, CF4, and CHF3.

Applications
  • Etch of Si
  • Etch of SiO2
  • Etch of SiNx
  • Etch of InP
  • Etch of Al, Cr, Ti, Nb, hafnia, alumina ....

- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page

NOTE: Au and Ag, Se, and Li compounds are NOT ALLOWED in the system