Difference between revisions of "Lesker PVD75 E-beam Evaporator"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
Line 27: Line 27:
  
 
== Resources ==
 
== Resources ==
[https://www.youtube.com/watch?v=OxkmP7Lr9Lo PVD-4 Training Video]
+
===== Training video =====
 +
Link: [https://www.youtube.com/watch?v=OxkmP7Lr9Lo PVD-4 Training Video]
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
* [https://repository.upenn.edu/scn_protocols/73/ QNF SOP]
+
Link: [https://repository.upenn.edu/scn_protocols/73/ QNF SOP]

Revision as of 08:40, 14 September 2022


Lesker PVD75 E-Beam/Thermal Evaporator
PVD-04.jpeg
Tool Name Lesker PVD75 E-Beam/Thermal Evaporator
Instrument Type Deposition
Staff Manager Jason (jarohr@seas.upenn.edu)
Lab Location Bay 2
Tool Manufacturer Kurt J. Lesker
Tool Model PVD75
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone 8-9748
SOP Link SOP

Description

The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool. The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd via e-beam evaporation.


Films
  • Ti
  • Cr
  • Au
  • Pd

Resources

Training video

Link: PVD-4 Training Video

SOPs & Troubleshooting

Link: QNF SOP