Difference between revisions of "Au (gold)"
Jump to navigation
Jump to search
(Created page with "==Equipment== ===Deposition Equipment=== * '''PVD-02:''' Lesker PVD75 E-Beam/Thermal Evaporator * '''PVD-03:''' Lesker PVD75...") |
|||
| Line 34: | Line 34: | ||
{| class="wikitable" | {| class="wikitable" | ||
! rowspan=2 | PVD Tool | ! rowspan=2 | PVD Tool | ||
| − | ! colspan=3 | Cathode 1&3 (DC) | + | ! colspan=3 | Cathode 1 & 3 (DC) |
! rowspan=2 | Recorded | ! rowspan=2 | Recorded | ||
|- | |- | ||
Revision as of 13:11, 9 May 2024
Equipment
Deposition Equipment
- PVD-02: Lesker PVD75 E-Beam/Thermal Evaporator
- PVD-03: Lesker PVD75 DC/RF Sputterer
- PVD-04: Lesker PVD75 E-beam Evaporator
- PVD-05: Denton Explorer14 Magnetron Sputterer
Etching
Applications
Processes
Sputter Deposition Rates
| PVD Tool | Cathode 2 (DC; high mag) | Recorded | Cathode 3 (DC) | Recorded | Cathode 4 (DC; high mag) | Recorded | ||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Pressure | Power | Rate | Pressure | Power | Rate | Pressure | Power | Rate | ||||
| PVD-03 | 4 mTorr | 140 W | 3.1 Å s-1 | 3 mTorr | 140 W | 2.5 Å s-1 | 03/06/23 | 5 mTorr | 140 W | 3.1 Å s-1 | ||
| PVD Tool | Cathode 1 & 3 (DC) | Recorded | ||
|---|---|---|---|---|
| Pressure | Power | Rate | ||
| PVD-05 | 3 mTorr | 140 W | 4.6 Å s-1 | |