Difference between revisions of "Oxford Cobra ICP Etcher"
Jump to navigation
Jump to search
(7 intermediate revisions by 2 users not shown) | |||
Line 7: | Line 7: | ||
| imagecaption = | | imagecaption = | ||
| Instrument_Type = Etch | | Instrument_Type = Etch | ||
− | | Staff_Manager = | + | | Staff_Manager = [[Lucas Barreto | Lucas Barreto]] |
| Lab_Location = Bay 2 | | Lab_Location = Bay 2 | ||
| Tool_Manufacturer = Oxford Instruments | | Tool_Manufacturer = Oxford Instruments | ||
| Tool_Model = Cobra PlasmaPro 100 | | Tool_Model = Cobra PlasmaPro 100 | ||
− | | | + | | NEMO_Designation = DE-05 |
| Lab_Phone = 215-898-9748 | | Lab_Phone = 215-898-9748 | ||
| SOP Link = [https://repository.upenn.edu/scn_sop/19/ SOP] | | SOP Link = [https://repository.upenn.edu/scn_sop/19/ SOP] | ||
Line 17: | Line 17: | ||
== Description == | == Description == | ||
− | Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures. | + | Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures. |
+ | * Max ICP power: 3 kW | ||
+ | * Max RF power: 200 W | ||
The tool is connected to the following gases: | The tool is connected to the following gases: | ||
Line 29: | Line 31: | ||
* Etch of Al, Cr, Ti, Nb, hafnia, alumina .... | * Etch of Al, Cr, Ti, Nb, hafnia, alumina .... | ||
- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page | - for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page | ||
+ | |||
+ | NOTE: Au and Ag, Se, and Li compounds are NOT ALLOWED in the system | ||
== Resources == | == Resources == |
Latest revision as of 14:15, 31 March 2025
![]() |
|
Tool Name | Oxford Cobra ICP Etcher |
---|---|
Instrument Type | Etch |
Staff Manager | Lucas Barreto |
Lab Location | Bay 2 |
Tool Manufacturer | Oxford Instruments |
Tool Model | Cobra PlasmaPro 100 |
NEMO Designation | DE-05 |
Lab Phone | 215-898-9748 |
SOP Link | SOP |
Description
Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures.
- Max ICP power: 3 kW
- Max RF power: 200 W
The tool is connected to the following gases: BCl3, Cl2, Ar, O2, SF6, CF4, and CHF3.
Applications
- Etch of Si
- Etch of SiO2
- Etch of SiNx
- Etch of InP
- Etch of Al, Cr, Ti, Nb, hafnia, alumina ....
- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page
NOTE: Au and Ag, Se, and Li compounds are NOT ALLOWED in the system