Difference between revisions of "Lesker PVD75 E-beam Evaporator"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
 
(One intermediate revision by the same user not shown)
Line 38: Line 38:
 
Link: [https://repository.upenn.edu/scn_sop/23/ SOP]
 
Link: [https://repository.upenn.edu/scn_sop/23/ SOP]
  
<pdf height="800">File:PVD 04 SOP_v07.pdf</pdf>
+
<pdf height="800">File:PVD04 SOP v07.pdf</pdf>

Latest revision as of 08:54, 4 September 2025


Lesker PVD75 E-Beam/Thermal Evaporator
PVD-04.jpeg
Tool Name Lesker PVD75 E-Beam/Thermal Evaporator
Instrument Type Physical vapor deposition
Staff Manager David Barth
Lab Location Bay 2
Tool Manufacturer Kurt J. Lesker
Tool Model PVD75
NEMO Designation PVD-04
Nearest Phone 215-898-9748
SOP Link SOP

Description

The tool

The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool. The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd. The tool also comes with a load-lock, allowing for fast and easy transfer of samples in and out of the system. While less flexible than the PVD-02 deposition system in terms of available materials, the PVD-04 is a much faster tool.

Available materials

The tool contains the following materials:

Deposition is limited to thin-film thicknesses of ~100 nm.

Resources

Training video

Link: PVD-4 Training Video

SOPs & Troubleshooting

Link: SOP