Difference between revisions of "Filmetrics Profilm3D"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(update to NEMO)
 
(5 intermediate revisions by 2 users not shown)
Line 4: Line 4:
 
| name = Filmetrics Profilm3D Optical Profilometer
 
| name = Filmetrics Profilm3D Optical Profilometer
 
| Tool_Name = Filmetrics Profilm3D Optical Profilometer
 
| Tool_Name = Filmetrics Profilm3D Optical Profilometer
| image = [[Image:MET-05.jpeg|300px]]
+
| image = [[Image:MET-05_new.jpeg|300px]]
 
| imagecaption =  
 
| imagecaption =  
 
| Instrument_Type = Metrology
 
| Instrument_Type = Metrology
| Staff_Manager = David Barth
+
| Staff_Manager = [[David Barth | David Barth]]
 
| Lab_Location = Cleanroom Corridor
 
| Lab_Location = Cleanroom Corridor
 
| Tool_Manufacturer = Filmetrics
 
| Tool_Manufacturer = Filmetrics
 
| Tool_Model = Profilm3D
 
| Tool_Model = Profilm3D
| Iris_Designation = MET-05
+
| NEMO_Designation = MET-05
 
| Lab_Phone = XXXXX
 
| Lab_Phone = XXXXX
| SOP Link =   
+
| SOP Link =  [https://repository.upenn.edu/server/api/core/bitstreams/c3892eaf-4315-4adf-bbd4-803c69ccd4dc/content SOP]
 
}}
 
}}
  
Line 20: Line 20:
 
== Description ==
 
== Description ==
  
The Profilm3D is an optical profilometer capable of white light interferometry (WLI), green light interferometry (GLI), and phase shift interferometry (PSI). It can measure surface topography, roughness, and step heights from 1 nm up to 10 mm. The tool currently has a 10x interferometry objective with a field of view ~2x2mm.
+
The Profilm3D is an optical profilometer capable of white light interferometry (WLI), green light interferometry (GLI), and phase shift interferometry (PSI). It can measure surface topography, roughness, and step heights from 1 nm up to 10 mm. The tool has two Mirau interferometry objectives: a 10x objective with a field of view ~2x2mm for high speed and large area measurements and a 50x objective for spatial resolution up to 0.176 μm.
  
 
===== Applications =====
 
===== Applications =====
Line 32: Line 32:
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
*
+
*[https://repository.upenn.edu/server/api/core/bitstreams/c3892eaf-4315-4adf-bbd4-803c69ccd4dc/content SOP]

Latest revision as of 13:18, 3 January 2024


Filmetrics Profilm3D Optical Profilometer
MET-05 new.jpeg
Tool Name Filmetrics Profilm3D Optical Profilometer
Instrument Type Metrology
Staff Manager David Barth
Lab Location Cleanroom Corridor
Tool Manufacturer Filmetrics
Tool Model Profilm3D
NEMO Designation MET-05
Lab Phone XXXXX
SOP Link SOP


Description

The Profilm3D is an optical profilometer capable of white light interferometry (WLI), green light interferometry (GLI), and phase shift interferometry (PSI). It can measure surface topography, roughness, and step heights from 1 nm up to 10 mm. The tool has two Mirau interferometry objectives: a 10x objective with a field of view ~2x2mm for high speed and large area measurements and a 50x objective for spatial resolution up to 0.176 μm.

Applications
  • Step height measurements
  • Surface roughness measurements
  • 3D mapping of surfaces


Resources

SOPs & Troubleshooting