* SiN<sub>x</sub> deposition rate of the standard recipe on the tool is ~ 490 nm/hour with thin film stress of ~ 60 MPa for a 1-hour run. The films deposited via LPCVD have a higher resistance towards CF4 etch and make better etch masks compared to those deposited using Singh Center's standard SiN<sub>x</sub> recipe on the PECVD . In an RIE system with CF4 etch, LPCVD silicon nitride is etched at the rate of 50 nm/min vs 80 nm/min for PECVD silicon nitride (CF4 recipe can be found under the Oxford 80+ page -- DE-04). The etch rate for LPCVD silicon nitride film in 49% HF at room temperature is ~ 2.5 nm/min.
 
  
 
== Resources ==
 
== Resources ==

Revision as of 11:37, 19 September 2022


Sandvik Furnace Stack
CVD-02.jpeg
Tool Name Sandvik Furnace Stack
Instrument Type Deposition
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer Ultratech/Cambridge
Tool Model S200
NEMO Designation {{{NEMO_Designation}}}
Lab Phone 215-898-9736
SOP Link SOP

Description

The Sandvik LPCVD consists of 4 furnace tubes:

Tube 1: Wet/Dry Silicon Oxide growth. Wet/Dry oxide: This tube uses the Si substrate to grow SiO2. Wet oxide refers to the use of water vapor as the source of oxygen and dry oxide uses O2 gas. Since water molecules can penetrate through the substrate more, wet oxide technique results in thicker oxides and faster growth rate. Wet oxide deposition on the tool is limited to 5 hours.

Tube 2: Low Stress Silicon Nitride deposition. This tube is designated to low stress silicon nitride.

Tube 3: Clean anneal. This tube is an RCA clean wafer only anneal tube, with N2 and H2N2 gases.

Tube 4: General anneal. This tube is a general anneal tube, with N2 and H2N2 gases

Applications
  • Wet/Dry Silicon Oxide deposition
  • Low Stress Silicon Nitride deposition
  • Annealing with N2 or H2N2 gases