Difference between revisions of "Jandel Multi Height Four Point Probe"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(Created page with "Category:Metrology {{EquipmentInfo | name = Jandel Multi Height Four Point Probe | Tool_Name = Jandel Multi Height Four Point Probe | image = 300px...")
 
 
(6 intermediate revisions by 4 users not shown)
Line 1: Line 1:
[[Category:Metrology]]
+
[[Category:Characterization]][[Category:Equipment]]
  
 
{{EquipmentInfo
 
{{EquipmentInfo
Line 6: Line 6:
 
| image = [[Image:MET-08.jpeg|300px]]
 
| image = [[Image:MET-08.jpeg|300px]]
 
| imagecaption =  
 
| imagecaption =  
| Instrument_Type = Metrology
+
| Instrument_Type = Electrical Characterization
| Staff_Manager = Sam Azadi
+
| Staff_Manager = [[Lucas Barreto | Lucas Barreto]]
| Lab_Location = Bay 2
+
| Lab_Location = Bay 4
 
| Tool_Manufacturer = Jandel
 
| Tool_Manufacturer = Jandel
 
| Tool_Model = Four Point Probe
 
| Tool_Model = Four Point Probe
| Iris_Designation = MET-08
+
| NEMO_Designation = MET-08
 
| Lab_Phone = XXXXX
 
| Lab_Phone = XXXXX
 
| SOP Link = [ NA]
 
| SOP Link = [ NA]
Line 27: Line 27:
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
* [ NA]
+
* [NA - staff assisted use only]

Latest revision as of 12:35, 28 July 2025


Jandel Multi Height Four Point Probe
MET-08.jpeg
Tool Name Jandel Multi Height Four Point Probe
Instrument Type Electrical Characterization
Staff Manager Lucas Barreto
Lab Location Bay 4
Tool Manufacturer Jandel
Tool Model Four Point Probe
NEMO Designation MET-08
Nearest Phone XXXXX
SOP Link [ NA]

Description

The system allows probing of wafers, ingots, or samples of widely varying dimensions. A locking mechanism allows the arm to be moved up and down the steel pole and locked to suit any sample height. A plug attached to the arm prevents the wiring from getting entangled with samples, fingers etc. The system utilizes a Jandel Cylindrical probe head.

Applications
  • Material resistivity measurements


Resources

SOPs & Troubleshooting
  • [NA - staff assisted use only]