|AZ422 MIF || AZ Materials/Merck || 0.21N TMAH (Metal Ion Free) w/ Surfactant || Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) || || MF321, TMAH 0.26N | |AZ422 MIF || AZ Materials/Merck || 0.21N TMAH (Metal Ion Free) w/ Surfactant || Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) || || MF321, TMAH 0.26N | ||
|- | |- | ||
| − | | AZ400K|| AZ Materials/Merck || Potassium Borates (Metal Ion Bearing) || Strong Base -- Irritant, Corrosive || | + | | AZ400K|| AZ Materials/Merck || Potassium Borates (Metal Ion Bearing) || Strong Base -- Irritant, Corrosive || Thick Photoresists (AZP4620), Mask Plates (AZ1500) -- Manually dilute 1:3 or 1:4 with DI water || |
|- | |- | ||
| SU-8 Developer || MicroChem/Kayaku || PGMEA (1-methoxy-2-propanol acetate) || Organic Solvent -- Flammable || SU-8, HARE SQ, IP-Dip || SQ Developer | | SU-8 Developer || MicroChem/Kayaku || PGMEA (1-methoxy-2-propanol acetate) || Organic Solvent -- Flammable || SU-8, HARE SQ, IP-Dip || SQ Developer | ||
Revision as of 12:08, 24 October 2023
The following are developers you may encounter in the QNF wet benches.
| Name | Manufacturer | Chemical Composition | Hazards | Use | Alternatives |
|---|---|---|---|---|---|
| TMAH 0.26N | KemLab | 0.26N TMAH (Metal Ion Free) | Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) | Photoresists, Liftoff Resists | CD-26, AZ300MIF |
| CD-26 | Microposit/Dupont | 0.26N TMAH (Metal Ion Free) | Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) | Photoresists, Liftoff Resists | TMAH 0.26N (preferred), AZ300MIF |
| AZ300 MIF | AZ Materials/Merck | 0.26N TMAH (Metal Ion Free) | Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) | Photoresists, Liftoff Resists | TMAH 0.26N (preferred), CD-26 |
| CD-26A | Microposit/Dupont | 0.26N TMAH (Metal Ion Free) w/ Surfactant | Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) | AZ917MIF, TMAH 0.26N, CD-26, AZ300MIF | |
| AZ917 MIF | AZ Materials/Merck | 0.26N TMAH (Metal Ion Free) w/ Surfactant | Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) | CD-26A, TMAH 0.26N, CD-26, AZ300MIF | |
| MF321 | Microposit/Dupont | 0.21N TMAH (Metal Ion Free) w/ Surfactant | Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) | AZ422 MIF, TMAH 0.26N | |
| AZ422 MIF | AZ Materials/Merck | 0.21N TMAH (Metal Ion Free) w/ Surfactant | Strong Base -- Toxic, Irritant (can cause chemical burns, lethal for high surface areas) | MF321, TMAH 0.26N | |
| AZ400K | AZ Materials/Merck | Potassium Borates (Metal Ion Bearing) | Strong Base -- Irritant, Corrosive | Thick Photoresists (AZP4620), Mask Plates (AZ1500) -- Manually dilute 1:3 or 1:4 with DI water | |
| SU-8 Developer | MicroChem/Kayaku | PGMEA (1-methoxy-2-propanol acetate) | Organic Solvent -- Flammable | SU-8, HARE SQ, IP-Dip | SQ Developer |
| SQ Developer | KemLab | PGMEA (1-methoxy-2-propanol acetate) | Organic Solvent -- Flammable | HARE SQ, SU-8, IP-Dip | SU-8 Developer |
| O-Xylene | N/A | O-Xylene | Organic Solvent -- Flammable, Irritant | ZEP520 | Amyl Acetate (preferred) |