Difference between revisions of "Oxford Cobra ICP Etcher"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
Line 32: Line 32:
 
- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page
 
- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page
  
NOTE: Au and Ag, and Se compounds are NOT ALLOWED in the system
+
NOTE: Au and Ag, Se, and Li compounds are NOT ALLOWED in the system
  
 
== Resources ==
 
== Resources ==

Revision as of 14:33, 6 September 2023


Oxford Cobra ICP Etcher
DE-05.jpeg
Tool Name Oxford Cobra ICP Etcher
Instrument Type Etch
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer Oxford Instruments
Tool Model Cobra PlasmaPro 100
NEMO Designation {{{NEMO_Designation}}}
Lab Phone 215-898-9748
SOP Link SOP

Description

Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures.

  • Max ICP power: 3 kW
  • Max RF power: 200 W

The tool is connected to the following gases: BCl3, Cl2, Ar, O2, SF6, CF4, and CHF3.

Applications
  • Etch of Si
  • Etch of SiO2
  • Etch of SiNx
  • Etch of InP
  • Etch of Al, Cr, Ti, Nb, hafnia, alumina ....

- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page

NOTE: Au and Ag, Se, and Li compounds are NOT ALLOWED in the system

Resources

SOPs & Troubleshooting