Uploads by Azadi

Jump to navigation Jump to search

This special page shows all uploaded files.

File list
Date Name Thumbnail Size Description Versions
16:37, 19 October 2022 Alumina.png (file)
Error creating thumbnail: Error code: 25
287 KB ALD alumina process control_150C 1
16:41, 19 October 2022 HfO2.png (file)
Error creating thumbnail: Error code: 25
281 KB HfO2 process control 150C 1
09:22, 26 October 2022 Hafnia Oct6.jpg (file) 423 KB   1
09:28, 26 October 2022 Alumina Oct6.jpg (file) 446 KB   1
15:32, 28 November 2022 Sio2 dep on cvd-01.jpg (file) 416 KB   1
15:33, 28 November 2022 Sinx dep rate on cvd-01.jpg (file) 402 KB   1
10:56, 6 December 2022 600cyc .4 sec 8 sec dec 6 2022.png (file) 101 KB   1
11:00, 22 May 2024 DE06 SOP v03.pdf (file) 39.03 MB   1
09:45, 18 June 2024 DE04 PECVD SiO2 rate etch via CHF3O2.png (file) 4.32 MB DE04 etch rate for PECVD SiO2 using CHF3 and O2 1
14:33, 30 July 2024 RIE CF4 etch rate 2min SiN LPCVD 07292024.png (file) 95 KB LPCVD SiNx with CF4 in RIE 1
14:44, 16 September 2024 SiN etch on DE-04.png (file) 2.12 MB   2
14:56, 16 September 2024 SiO2 etch via DE04 CHF3 O2.png (file) 1.44 MB   1
12:01, 6 November 2024 IBE.jpg (file) 2.34 MB IBE 1
12:12, 6 November 2024 DE01 SOP.pdf (file) 27.57 MB DE01_SOP 1