QNF Soft Litho Fabrication Service

From The Singh Center for Nanotechnology Wiki
Jump to navigation Jump to search


About

Example soft lithography master fabricated in the QNF -- contains multiple designs including gradient generators and an image of the Singh Center for Nanotechnology

The QNF provides a fabrication service of soft lithography masters for the purposes of PDMS molding/casting and associated applications, such as microfluidic device production and micro-contact printing. Each master is custom fabricated by our technical staff in the QNF cleanroom using SU-8 negative epoxy resist (e.g., HARE SQ) on a 4” silicon wafer.

This service was created to address a need communicated by our colleagues at Penn School of Medicine and the Children’s Hospital of Philadelphia, where the onboarding and training time of a new cleanroom user is often too significant an investment for a lab needing only a couple masters requiring minimal fabrication once every few years.

Services

Our standard master fabrication process includes single layer photolithography (one feature height, no alignment) with basic quality inspection and characterization. Standard feature sizes/standard parameters include:

  • Feature widths/lengths larger than 20 μm (within +/- 10% target value)
  • Feature heights/channel depths up to 100 μm (within +/- 20% target value)
  • Aspect ratios (width to height) up to 1:4

Other services may be requested but are subject to additional review. These include two-layer masters, design assistance, and process optimization -- such as for smaller feature sizes, thicker layer heights, tighter tolerances, and specialty alignment.

IMPORTANT NOTE: Service availability is currently limited to internal and external academic requests. We do not currently have the capability to fulfill requests from corporate or private sources.

Pricing

Fee (Academic Rate)
Master, Single Layer $ 1060
Master, Two Layers $ 3295
Staff Support $ 55 / hour

Design assistance as well as consultations outside of the initial 30-min meeting will be billed as staff support. The per-master price is based on a comprehensive review of the required materials, equipment, hours and reflects the true costs of cleanroom fabrication. Additional fabrication services, such as calibration tests, will be an additional fee quoted based on individual processing needs. All pricing and tool availability are subject to change over time.

Getting Started

1. Create your design!

h = feature height/layer thickness, w = feature width, d = spacing of features
Examples of closed polygons (on left) and unrecognized shapes (on right)
Solid line = distance between devices (ideal>15mm), dashed line = pattern limit to maintain proper distance to edge of wafer (ideal>10mm)

Having a clear final design concept to minimize possible reworking of the design, which will incur extra staff charges. If you have any questions about the design, you may reach out to QNF staff about available assistance.

Design Considerations

Feature sizes

  • Height (h) < 100μm -- limited by available resist material and associated processing
  • Width (w) > 10um, spacing (d) > 10μm -- limited by photolithography process on thicker resist
  • Aspect ratios (w:h) < 1:4 -- tall narrow structures can have less stability and be more prone to breakage or delamination

Formatting

  • All features must be closed polygons to be readable as the intended shape
  • GDS format is preferred -- DXF is acceptable for discussion purposes, but conversion to GDS for fabrication will incur staff charges at $55/hour

Leave enough space to cut out the PDMS!

  • Designs should be > 10mm from the edge of the substrate (if using a 4" wafer, everything should fit within a 90mm diameter circular area)
  • Individual devices should be spaced > 15mm apart


2. Fill out our request form.

Make sure to include your design files, specifications and other needs. Staff will review your design and requested parameters ahead of the consultation to help get a sense of the feasibility, expected costs, and if there is any other information needed.

Complete specifications include:

  • Feature sizes (minimum and typical)
  • Channel depths and widths
  • Critical dimensions with tolerances

IMPORTANT: It is important that you have a final design or otherwise indicate that you wish to discuss design with QNF Staff. If the design changes between your initial contact and your consultation, you are not guaranteed to have adequate staff review time, resulting in an inefficient consultation.


3. Initial consultation (30 min)

After reviewing your request, someone from our team will contact you to schedule a consultation. During this meeting our team will

  1. Review your design for feasibility with our processes and capabilities
  2. Discuss specifications and clarify any ambiguities or questions
  3. Identify potential issues and suggest optimizations if needed
  4. Estimate timeline and confirm pricing for your specific project
  5. Determine next steps: whether ready for quote and fabrication, needing design modifications (may incur $55/hour charges), or scheduling an additional consultation to finalize details

Come Prepared!

This 30-minute initial consultation is the one complimentary consultation included with your service and is a valuable opportunity to get complimentary design review and fabrication guidance. To make the most of this time:

  • Know your critical specifications and tolerances
  • Prepare specific questions about feasibility or design concerns
  • Gather any other helpful information
    • Sketches or diagrams of your design
    • Examples of similar devices you've used
    • Information about your PDMS molding process
    • Any previous fabrication attempts and their outcomes.


4. Submit the NEMO Access Request Form

Payment processing will be managed through our billing system in NEMO. Submit the NEMO Access Request Form to begin account setup. Any questions can be directed to admin[at]nano.upenn.edu


5. Quote / Service Agreement

Staff will follow up with the official quote. Each quote which must be signed and returned as part of accepting each request before fabrication begins. By signing the quote, you accept the quoted cost as well as our service agreement. The agreement text is included in each quote -- an example quote with this text can be found here


6. Fabrication begins!

Fabrication begins only after receipt of signed quote and confirmation of active NEMO account for billing.

Delivery Time

Turnaround time varies based on tool availability and master complexity. An estimate should be provided during the consultation. A more detailed timeline can be provided upon request.

Making Changes

Any changes to the fabrication request will require additional charges or order cancellation. Once fabrication begins, any modification or cancellation of an order will result in charges for any processing already executed for the previous request.

Additional Information

Payment

Payment processing is managed through our billing system in NEMO at nemo.nano.upenn.edu

Limitations

Although we strive to minimize fabrication issues, we cannot guarantee specific defect density thresholds, exact sidewall smoothness or angle, precise feature depth tolerances, nor suitability for any particular application.

If the demand of your lab surpasses what QNF staff can reasonably provide through this fabrication service (e.g. high volume of requests or more intensive process development), you will instead be provided the option to sign up as a standard QNF user to continue these projects. For more information about soft lithography masters and processing, see our Soft Lithography wiki page.

Publications Policy

If you publish on devices or work done using this service, please add an acknowledgement or line of text stating the following: A portion of this work was carried out in part at the Singh Center for Nanotechnology, which is supported by the NSF National Nanotechnology Coordinated Infrastructure Program under grant NNCI-2025608. This is important for the continued success of our facility.

In addition, process knowledge gained from conversations, advice and brainstorming sessions, as well as fabrication executed by QNF staff may also constitute significant "intellectual contribution", and warrant authorship, or be worthy of an acknowledgement. Feel free to contact us if you would like to discuss, and thank you for understanding.

Have Questions?

Contact us at qnf-fabservices@engineering.upenn.edu