==Processes==
 
==Processes==
  
Gold is NOT allowed in the following tools: [[Oxford PlasmaLab 100 PECVD | CVD-01]],  
+
Gold is NOT allowed in the following tools: [[Oxford PlasmaLab 100 PECVD | CVD-01]], [[Cambridge Nanotech S200 ALD | ALD-01]], [[SPTS Si DRIE | DE-03]], [[Oxford 80 Plus RIE | DE-04]], [[Oxford Cobra ICP Etcher
 +
| DE-05]],  
  
 
===Sputter Deposition Rates===
 
===Sputter Deposition Rates===

Revision as of 14:39, 9 May 2024

Gold is noble transition metal with atomic number 79 and symbol Au. Gold has a very high density and very low reactivity. It also has excellent thermal and electrical conductivity.

Equipment

Deposition Equipment

Etching Equipment

Applications

Processes

Gold is NOT allowed in the following tools: CVD-01, ALD-01, DE-03, DE-04, [[Oxford Cobra ICP Etcher

| DE-05]], 

Sputter Deposition Rates

PVD Tool Cathode 2 (DC; high mag) Recorded Cathode 3 (DC) Recorded Cathode 4 (DC; high mag) Recorded
Pressure Power Rate Pressure Power Rate Pressure Power Rate
PVD-03 4 mTorr 140 W 3.1 Å s-1 3 mTorr 140 W 2.5 Å s-1 03/06/23 5 mTorr 140 W 3.1 Å s-1
PVD Tool Cathodes 1 & 3 (DC) Recorded
Pressure Power Rate
PVD-05 3 mTorr 140 W 4.6 Å s-1

PVD-05 Master Recipe:

Step T006 is the deposition step.

Step Number T000 T001 T002 T003 T004 T005 T006 T007 T008 T009 T010 T011 T012 T013
Step Time (sec) 5 30 30 30 30 30 [dep] 30 30 30 30 30 300 5
Min Vacuum Setpoint (Torr)
Gas - (PID or Fixed) PID PID PID PID PID PID PID PID PID PID PID
Gas - PID Master Gas Select 1 1 1 1 1 1 1 1 1 1 1
Gas1 - Setpoint (sccm) 10 10 10 10 10 10 10 10 10 10 10
Gas2 - Setpoint (sccm)
Gas PID Pressure (mTorr) 3 3 3 3 3 3 3 3 3 3 3
RF Source - Sputter (Watts)
RF Source - Cathode Select
RF Source - Shutter
DC 1 Source - Sputter (Watts) 25 50 75 100 125 140 120 100 80 60 25
DC 1 Source - Cathode Select 1 1 1 1 1 1 1 1 1 1 1
DC 1 Source - Shutter Open
DC 2 Source - Sputter (Watts)
DC 2 Source - Shutter
Pressure Control (Throttle) Yes Yes Yes Yes Yes Yes Yes Yes Yes Yes Yes Yes
Ignition Pressure (mTorr)
Rotation Speed (0-100%) 50 50 50 50 50 50 50 50 50 50 50 50 50
End Process (Yes) Yes