Difference between revisions of "Anatech SCE-106 Barrel Asher"
Jump to navigation
Jump to search
(update tool owner) |
(update location to Bay 6) |
||
Line 8: | Line 8: | ||
| Instrument_Type = Soft Lithography | | Instrument_Type = Soft Lithography | ||
| Staff_Manager = [[Ana Cohen | Ana Cohen]] | | Staff_Manager = [[Ana Cohen | Ana Cohen]] | ||
− | | Lab_Location = Bay | + | | Lab_Location = Bay 6 |
| Tool_Manufacturer = Anatech | | Tool_Manufacturer = Anatech | ||
| Tool_Model = SCE-106 | | Tool_Model = SCE-106 |
Revision as of 16:22, 12 March 2024
Tool Name | Anatech SCE-106 Barrel Asher |
---|---|
Instrument Type | Soft Lithography |
Staff Manager | Ana Cohen |
Lab Location | Bay 6 |
Tool Manufacturer | Anatech |
Tool Model | SCE-106 |
NEMO Designation | DE-07 |
Lab Phone | XXXXX |
SOP Link | SOP |
Description
Anatech USA’s SCE-100 Series Inductively Coupled (ICP) Plasma systems are extremely effective for a Plasma Ashing process to remove organics prior to thin film deposition and/or chemical analysis of remaining inorganics.
Process gases are CF4, O2, Ar and N2. Sample sizes are pieces to 150 mm round wafers.
Applications
- Removal of photoresist
- Removal of organic materials