MPT Corp. RTP-600S Rapid Thermal Annealer
Revision as of 13:35, 2 May 2022 by Dsbarth (talk | contribs) (Changed protection level for "MPT Corp. RTP-600S Rapid Thermal Annealer" ([Edit=Allow only autoconfirmed users] (indefinite) [Move=Allow only autoconfirmed users] (indefinite)))
![]() |
|
Tool Name | MPT Corp. RTP-600S Rapid Thermal Annealer |
---|---|
Instrument Type | Back End |
Staff Manager | David Barth |
Lab Location | Bay 2 |
Tool Manufacturer | MPT Corp. |
Tool Model | RTP-600S |
NEMO Designation | {{{NEMO_Designation}}} |
Lab Phone | XXXXX |
SOP Link | SOP |
Description
The RTP-600S system is an advanced bench-top rapid thermal processing system with multi-gas capabilities. The system processes wafers up to 6″ in diameter. The integrated process control system features real-time graphics, recipe management, data acquisition and display and has a comprehensive diagnostic function.
The system is configured for ≤800°C processing with thermocouple and has the option to flow in nitrogen as a process gas.
Applications
- Rapid thermal annealing of thin-films.