Description

The ABM Mask Aligner is a manual and versatile mask aligner with top-side alignment and substrate capabilities from 100mm down to small pieces. Requires a 5" mask or 5" glass plate with film mask.

Applications

Tool is used primarily for SU8 exposure. It can also be used for aligning PDMS components for PDMS-to-PDMS bonding.

Exposure time = dose (mJ/cm^2) / intensity (mW/cm^2) Dose can be determined from the resist data sheet. See table below for intensities.

To obtain vertical sidewalls with a Cr glass mask, use the long pass filter (PL-360-LP) which eliminates UV emission below 350nm. Do not use with film masks. Inherent defects in film masks will be accentuated, resulting in worse results.

mW/cm^2 % of output
NO MASK ~10 100%
GLASS MASK ~9 87.5%
GLASS + FILM MASK ~7 68.5%
GLASS + LP FILTER ~5 47%
GLASS + FILM + LP FILTER ~4 37%

More information about Soft Lithography processing can be found under Process Resources