Lesker Nano-36 Thermal Evaporator
Revision as of 16:30, 28 March 2022 by Trevinoj (talk | contribs) (Created page with "Category:Deposition {{EquipmentInfo | name = Lesker Nano-36 Thermal Evaporator | Tool_Name = Lesker Nano-36 Thermal Evaporator | image = 300px | ima...")
![]() |
|
Tool Name | Lesker Nano-36 Thermal Evaporator |
---|---|
Instrument Type | Deposition |
Staff Manager | David Barth |
Lab Location | Bay 2 |
Tool Manufacturer | Kurt J. Lesker |
Tool Model | Nano-36 |
NEMO Designation | {{{NEMO_Designation}}} |
Lab Phone | XXXXX |
SOP Link | SOP |
Description
The Kurt J. Lesker Nano36 will evaporate a metal film under high vacuum while measuring the thickness in-sit by a thickness monitor. Up to four different materials can be loaded in one batch, and the evaporation sources are sufficiently isolated from each other by shields to prevent cross contamination. The wafer platen can accommodate sizes up to 150 mm.
Films
- Ti
- Ni
- Cr
- Fe
- Pb
- NiCr
- Deposition of other films can be made available upon request