Veeco Fiji G2
ALD-03.jpeg
Tool Name Veeco Figi G2
Instrument Type Deposition
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer Veeco
Tool Model Fiji G2
NEMO Designation ALD-02
Lab Phone 215-898-9736
SOP Link SOP

Description

Fiji is a plasma and thermal ALD equipped with high-speed pneumatic pulse valves to enable our unique Exposure Mode for thin film deposition on Ultra High Aspect Ratio substrates. This proven precision thin film coating methodology can be used to deposit conformal, uniform films on substrates with aspect ratios of greater than > 2000:1. Savannah is capable of holding substrates of different sizes up to 200mm. The Fiji thin film deposition system is equipped with TMA, DEZ.

Films
  • Al2O3
  • ZnO