Difference between revisions of "Lesker PVD75 DC/RF Sputterer"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
Line 80: Line 80:
 
* Please consult with staff
 
* Please consult with staff
  
== Resources ==
+
== Important resources ==
  
[https://docs.google.com/forms/d/e/1FAIpQLScwWE1RvqXfH9hwqrQcYDLpgN6L9uNGdaZlq5Hw3NjqXng30g/viewform Target Request Form]
+
===== Target request form =====
  
===== SOPs & Troubleshooting =====
+
* [https://docs.google.com/forms/d/e/1FAIpQLScwWE1RvqXfH9hwqrQcYDLpgN6L9uNGdaZlq5Hw3NjqXng30g/viewform Link to Google form]
 +
 
 +
===== SOPs & troubleshooting =====
 
* [https://www.seas.upenn.edu/~nanosop/PVD75_Sputtering_SOP.htm SOP]
 
* [https://www.seas.upenn.edu/~nanosop/PVD75_Sputtering_SOP.htm SOP]
  
 
* [https://upenn.box.com/s/duex4o7xnhoq4dbqoo51aaij1o1b44mk PVD-03 Open Load SOP]
 
* [https://upenn.box.com/s/duex4o7xnhoq4dbqoo51aaij1o1b44mk PVD-03 Open Load SOP]
  
===== Process Data =====
+
===== Process data =====
 
* [https://upenn.box.com/s/lujbua3msga3313fntajkw3bcwh0d63w PVD-03 Recipes]
 
* [https://upenn.box.com/s/lujbua3msga3313fntajkw3bcwh0d63w PVD-03 Recipes]
 
* [https://www.angstromsciences.com/sputtering-yields Sputter Yield Chart]
 
* [https://www.angstromsciences.com/sputtering-yields Sputter Yield Chart]
 
:: Note: The sputter yield chart can be useful for estimating approximately what rate to expect from materials, but the rate given is highly dependent on tool configuration and is not directly relevant
 
:: Note: The sputter yield chart can be useful for estimating approximately what rate to expect from materials, but the rate given is highly dependent on tool configuration and is not directly relevant

Revision as of 10:40, 8 July 2022


Lesker PVD75 DC/RF Sputterer
PVD-03.jpeg
Tool Name Lesker PVD75 DC/RF Sputterer
Instrument Type Deposition
Staff Manager David Barth
Lab Location Bay 2
Tool Manufacturer Kurt J. Lesker
Tool Model PVD75
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone XXXXX
SOP Link SOP

Tool description

The Kurt J. Lesker PVD75 Sputter system is configured with 4 sputter guns in the following configuration:

Target 1: RF power, insulating/conductive target
Target 2: DC power, magnetic/non-magnetic conductive target
Target 3: DC power, non-magnetic conductive target
Target 4: DC power, magnetic/non-magnetic conductive target

The system is cryo-pumped process chamber with an automated interface, wafer platen rotation and heating up to 550°C, accepting sample sized from pieces to 150 mm diameter wafers.

When choosing between PVD-03 and PVD-05, consider the following:

  • PVD-03 is a load-locked system so base pressure will be better (~5e-8 torr vs. ~5e-6 torr) and pumpdown times will be much faster compared with PVD-05, which is an open load system.
  • PVD-03 can handle one 6" wafer or one 4" wafer (or several smaller pieces) per run. PVD-05 has a large platen and can accept about four 4" wafers with good uniformity.
  • PVD-03 is in a sputter up configuration, which means the guns point up and the sample must be attached upside down. This is usually considered cleaner, but requires greater consideration for sample mounting. PVD-05 is in sputter down configuration, so samples can just be placed on the platen.
  • Magnetic materials can only be sputtered from PVD-03. PVD-05 does not have the necessary high mag sources

Deposition sources

Metals
  • Ag (Warning! Ag target must be cooled down for more than 15 min after deposition)
  • Al
  • Au
  • Co
  • Cr
  • Cu
  • Fe
  • Mn
  • Mo
  • Nb
  • Ni
  • Pd
  • Pt
  • Ti
  • W
Semiconductors & metalloids
  • Ge
  • Sb
  • Si
  • p-Si (boron-doped)
Oxides, fluorides & nitrides
  • Al2O3
  • AZO (ZnO2/Al2O3; transparent conductive oxide)
  • ITO (indium-doped tin oxide; transparent conductive oxide)
  • MgF2
  • MgO
  • NbN
  • Si3N4
  • SiO2
  • Ta2O5
  • TiO2
  • TiN
Alloys & ceramics
  • Al/Si (99/1)
  • Fe/Ge (81/19 & 83/17)
  • Ni/Fe
  • Ni/Cr (80/20)
  • YSZ (Yttria-stabilized zirconia)
Other targets
  • Please consult with staff

Important resources

Target request form
SOPs & troubleshooting
Process data
Note: The sputter yield chart can be useful for estimating approximately what rate to expect from materials, but the rate given is highly dependent on tool configuration and is not directly relevant