Tool Name | Woollam V-VASE Ellipsometer |
---|---|
Instrument Type | Metrology |
Staff Manager | Eric Johnston |
Lab Location | Bay 2 |
Tool Manufacturer | J. A. Woollam Co. |
Tool Model | V-Vase |
NEMO Designation | {{{NEMO_Designation}}} |
Lab Phone | XXXXX |
SOP Link | SOP |
Description
The V-VASE is a Variable Angle Spectroscopic Ellipsometer and features totally automated thin film characterization, high-precision angle, and a wide spectral range (240nm to 1700nm). It has a vertical sample mounting, automated sample mapping, and focused spot size. Some of the key benefits are: highest precision and accuracy of any Spectroscopic Ellipsometer, totally automated angle of incidence, nondestructive materials analysis, easily characterize all types of materials: semiconductors, dielectrics, polymers, metals, multilayers, and more
Applications
- Reflection and Transmission Ellipsometry
- Generalized Ellipsometry
- Reflectance (R) intensity
- Transmittance (T) intensity
- Cross-polarized R/T
- Depolarization
- Scatterometry
- Mueller-matrix