Difference between revisions of "Lesker Nano-36 Thermal Evaporator"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
m (Protected "Lesker Nano-36 Thermal Evaporator" ([Edit=Allow only administrators] (indefinite) [Move=Allow only administrators] (indefinite)) [cascading])

Revision as of 10:43, 29 April 2022


Lesker Nano-36 Thermal Evaporator
PVD-01.jpeg
Tool Name Lesker Nano-36 Thermal Evaporator
Instrument Type Deposition
Staff Manager David Barth
Lab Location Bay 2
Tool Manufacturer Kurt J. Lesker
Tool Model Nano-36
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone XXXXX
SOP Link SOP

Description

The Kurt J. Lesker Nano36 will evaporate a metal film under high vacuum while measuring the thickness in-sit by a thickness monitor. Up to four different materials can be loaded in one batch, and the evaporation sources are sufficiently isolated from each other by shields to prevent cross contamination. The wafer platen can accommodate sizes up to 150 mm.


Deposition Sources
  • Ti
  • Ni
  • Cr
  • Fe
  • Pb
  • NiCr
  • Deposition of other films can be made available upon request