Difference between revisions of "Nanoscribe Photonic Professional GT"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
Line 30: Line 30:
 
* Stage scanning range: 100 x 100 mm2
 
* Stage scanning range: 100 x 100 mm2
  
====Objectives====
+
{| class="wikitable" style="vertical-align:bottom;"
* 10x
+
|-
* 20x
+
! Objective
* 25x
+
! Standard Resin
* 63x
+
! Voxel size
 +
! Print field (radius)
 +
|-
 +
| 63x
 +
| IP-Dip2
 +
| ~0.2um
 +
| 100um
 +
|-
 +
| 25x
 +
| IP-S
 +
| ~0.6um
 +
| 200um
 +
|-
 +
| 10x
 +
| IP-Q
 +
| ~1.2um
 +
| 500um
 +
|}
 +
 
 +
'''Voxel =''' the smallest printable 3D volume, the 3D analogue of a 2D pixel. Single voxels are not mechanically stable. Multiple neighboring voxels/lines are recommended for stable structures.
 +
 
 +
'''Print field =''' the circular region an objective could write without moving the stage. Structures that exceed the print field of the objective must be split into blocks in Describe.
  
 
== Allowed Materials ==
 
== Allowed Materials ==

Revision as of 15:41, 7 November 2025


Nanoscribe Photonic Professional GT+
LW-02.jpeg
Tool Name Nanoscribe Photonic Professional GT+
Instrument Type Lithography
Staff Manager Ana Cohen
Lab Location Bay 6
Tool Manufacturer Nanoscribe
Tool Model Photonic Professional GT+
NEMO Designation LW-02
Nearest Phone XXXXX
SOP Link SOP

Description

The Nanoscribe Photonic Professional enables the fabrication of true 3D structures in the microscale via two-photon polymerization using a 780nm laser with ~100fs pulse, 80MHz repetition rate. This system allows for cutting-edge research and rapid prototyping in microfluidics, MEMS, microoptics, nanostructures and more.

Upgraded to GT+ in Dec 2024! Includes new housing with easier objective loading with 10x objective capability and greater print height (previously 3mm)

Key Features

  • Laser Power: 50-150mW
  • Print Height: Up to 8mm
  • Lateral resolution ~ 200 nm
  • Vertical resolution ~ 300 nm
  • Piezo scanning range: 300 x 300 x 300 μm3
  • Stage scanning range: 100 x 100 mm2
Objective Standard Resin Voxel size Print field (radius)
63x IP-Dip2 ~0.2um 100um
25x IP-S ~0.6um 200um
10x IP-Q ~1.2um 500um

Voxel = the smallest printable 3D volume, the 3D analogue of a 2D pixel. Single voxels are not mechanically stable. Multiple neighboring voxels/lines are recommended for stable structures.

Print field = the circular region an objective could write without moving the stage. Structures that exceed the print field of the objective must be split into blocks in Describe.

Allowed Materials

Substrates

  • 4" Si wafers (~500um thickness)
  • Silicon pieces, 25mmx25mmx700um or 25mmx25mmx550um
  • Nanoscribe ITO-coated Soda Lime, 25mmx25mmx700um -- available in the QNF Stockroom
  • Nanoscribe Fused Silica, 25mmx25mmx700um -- available in the QNF Stockroom

Resists

Other materials must have tool owner approval before use!

Training Protocol

1. Remote session on EBL-02 for the Describe conversion software, using your structure (90min)
2. In-person session on LW-02 (120min)
3. Qualification session on LW-02, where you run the tool with minimal input (~60min) -- must be done after previous two sessions are completed, cannot be done the same day as the in-person training

All should be requested through NEMO.

Resources

SOPs & Troubleshooting
Related Processing
References