Difference between revisions of "Keyence Profilometer"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(Created page with "Category:Characterization {{EquipmentInfo | name = Keyence Profilometer | Tool_Name = Keyence | image = 300px | imagecaption = | Instrument_Type = P...")
 
(filled out page with more information, titles and descriptions of manuals copied from operating guide)
 
Line 18: Line 18:
 
== Description ==
 
== Description ==
 
The Keyence VK-X3100 combines laser scanning confocal microscopy with white light/focus variation modes to measure 3D characteristics of surfaces, including roughness, planar dimensions, height, film thickness, and more. The tool includes objective lenses from 5X to 50X, allowing both low and high magnification work on a variety of surfaces.
 
The Keyence VK-X3100 combines laser scanning confocal microscopy with white light/focus variation modes to measure 3D characteristics of surfaces, including roughness, planar dimensions, height, film thickness, and more. The tool includes objective lenses from 5X to 50X, allowing both low and high magnification work on a variety of surfaces.
 +
 +
This tool is an ideal alternative to SEM when capturing large fields of view or measuring features due to its ability to scan and stitch large areas and its suite of 3D measurement tools. A copy of the data analysis program is available in the NCF computer room in 023.
 +
 +
To obtain good measurements, it is crucial that data is properly filtered before measuring. Some basic information on filtering and measurement modes are provided in the manuals, but these are not exhaustive documents.
 +
 +
== Manuals ==
 +
The Keyence comes with a collection of manuals to orient users to the basic operations and procedures for various data collection and analysis modes:
 +
 +
=== Collecting Data ===
 +
==== Gathering New Data Using Laser Confocal ====
 +
Detects height information using reflected laser intensity and the objective focus. May have reduced data quality and angular resolution at low magnifications.
 +
 +
==== Gathering New Data Using Focus Variation/White Light Interferometer ====
 +
Currently no Interferometry available. Focus Variation captures multiple optical images at different focal lengths and uses the change in contrast to determine shape information.
 +
 +
==== Gathering New Film Thickness Data ====
 +
Techniques for measuring film thickness, including permeable films and glass, as well as transparent coatings. Uses either laser confocal or spectral interference.
 +
 +
=== Analysis Techniques ===
 +
==== Process Image ====
 +
Basic processing and filtering procedures to be done before analysis.
 +
 +
==== Average Step Height Measurement (Flatness) ====
 +
A tool to determine height difference, maximum height, minimum height, and flatness.
 +
 +
==== Comparative Measurement ====
 +
A tool for direct comparison of 2 profile lines from different samples.
 +
 +
==== Plane Measurement ====
 +
A tool to measure various lengths, angles, diameters, etc.
 +
 +
==== Profile Measurement ====
 +
The function to measure the height, distance (length,) cross-sectional area, angle, R (arc,) etc. of a profile graph of any profile line (straight or curved.)
 +
 +
==== Surface Roughness Measurement ====
 +
Line, multiline, and surface roughness measurement according to ISO standards.
 +
 +
==== Volume and Area Measurement ====
 +
A tool to measure convex or concave volume, cross sectional area, and surface area.
 +
 +
=== Repeated Measurement Techniques ===
 +
==== Batch Analysis/Recommendation ====
 +
A useful technique for conducting measurements across several similar samples. Recommendation can be used to differentiate surfaces based on their surface texture.
 +
 +
==== Teaching Module ====
 +
Evaluate multiple measurement positions by changing the lens, measurement method, or measurement conditions. May be used as an inspection mode with a template file containing nominal values and tolerances.

Latest revision as of 13:33, 5 August 2024


Keyence Profilometer
Keyence.jpg
Tool Name Keyence
Instrument Type Profilometer
Staff Manager Nicole Bohn, Matt Brukman, Jamie Ford
Lab Location Singh 018
Tool Manufacturer Keyence
Tool Model Keyence VK-X3100
NEMO Designation Keyence Profilometer
Nearest Phone XXXXX
SOP Link Keyence Operating Guide

Description

The Keyence VK-X3100 combines laser scanning confocal microscopy with white light/focus variation modes to measure 3D characteristics of surfaces, including roughness, planar dimensions, height, film thickness, and more. The tool includes objective lenses from 5X to 50X, allowing both low and high magnification work on a variety of surfaces.

This tool is an ideal alternative to SEM when capturing large fields of view or measuring features due to its ability to scan and stitch large areas and its suite of 3D measurement tools. A copy of the data analysis program is available in the NCF computer room in 023.

To obtain good measurements, it is crucial that data is properly filtered before measuring. Some basic information on filtering and measurement modes are provided in the manuals, but these are not exhaustive documents.

Manuals

The Keyence comes with a collection of manuals to orient users to the basic operations and procedures for various data collection and analysis modes:

Collecting Data

Gathering New Data Using Laser Confocal

Detects height information using reflected laser intensity and the objective focus. May have reduced data quality and angular resolution at low magnifications.

Gathering New Data Using Focus Variation/White Light Interferometer

Currently no Interferometry available. Focus Variation captures multiple optical images at different focal lengths and uses the change in contrast to determine shape information.

Gathering New Film Thickness Data

Techniques for measuring film thickness, including permeable films and glass, as well as transparent coatings. Uses either laser confocal or spectral interference.

Analysis Techniques

Process Image

Basic processing and filtering procedures to be done before analysis.

Average Step Height Measurement (Flatness)

A tool to determine height difference, maximum height, minimum height, and flatness.

Comparative Measurement

A tool for direct comparison of 2 profile lines from different samples.

Plane Measurement

A tool to measure various lengths, angles, diameters, etc.

Profile Measurement

The function to measure the height, distance (length,) cross-sectional area, angle, R (arc,) etc. of a profile graph of any profile line (straight or curved.)

Surface Roughness Measurement

Line, multiline, and surface roughness measurement according to ISO standards.

Volume and Area Measurement

A tool to measure convex or concave volume, cross sectional area, and surface area.

Repeated Measurement Techniques

Batch Analysis/Recommendation

A useful technique for conducting measurements across several similar samples. Recommendation can be used to differentiate surfaces based on their surface texture.

Teaching Module

Evaluate multiple measurement positions by changing the lens, measurement method, or measurement conditions. May be used as an inspection mode with a template file containing nominal values and tolerances.