Difference between revisions of "K&S Wire Bonder"
Jump to navigation
Jump to search
(update to NEMO) |
|||
Line 7: | Line 7: | ||
| imagecaption = | | imagecaption = | ||
| Instrument_Type = Back End | | Instrument_Type = Back End | ||
− | | Staff_Manager = Eric Johnston | + | | Staff_Manager = [[Eric Johnston | Eric Johnston]] |
| Lab_Location = Bay 2 | | Lab_Location = Bay 2 | ||
| Tool_Manufacturer = Kulicke & Soffa | | Tool_Manufacturer = Kulicke & Soffa | ||
| Tool_Model = 4523 | | Tool_Model = 4523 | ||
− | | | + | | NEMO_Designation = BE-03 |
| Lab_Phone = XXXXX | | Lab_Phone = XXXXX | ||
| SOP Link = [https://www.seas.upenn.edu/~nanosop/Wire_Bonder_SOP.htm SOP] | | SOP Link = [https://www.seas.upenn.edu/~nanosop/Wire_Bonder_SOP.htm SOP] |
Revision as of 14:23, 3 January 2024
![]() |
|
Tool Name | K&S Wire Bonder |
---|---|
Instrument Type | Back End |
Staff Manager | Eric Johnston |
Lab Location | Bay 2 |
Tool Manufacturer | Kulicke & Soffa |
Tool Model | 4523 |
NEMO Designation | BE-03 |
Nearest Phone | XXXXX |
SOP Link | SOP |
Description
Aluminum and gold wire wedge bonder. It provides digital controls with semiautomatic bonding cycle, but manual alignment.
The bonder can be operated in auto cycle or manual mode. The auto cycle mode is the preferred mode for most applications. Stitch bonding can be performed in the auto cycle mode. The manual mode is useful when the elevation between subsequent bond-pairs is substantially different.
Applications
- Aluminum wedge wire bonding
- Gold wedge wire bonding