Difference between revisions of "Oxford PlasmaLab 100 PECVD"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
Line 110: Line 110:
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
* [https://repository.upenn.edu/scn_sop/6/ QNF SOP]
+
* [https://repository.upenn.edu/scn_sop/5/ QNF SOP]
  
 
===== Protocols and Reports =====
 
===== Protocols and Reports =====

Revision as of 11:43, 18 November 2022


Oxford PlasmaLab 100 PECVD
CVD-01.jpeg
Tool Name Oxford PlasmaLab 100 PECVD
Instrument Type Deposition
Staff Manager Sam Azadi
Lab Location Bay 1
Tool Manufacturer Oxford
Tool Model PlasmaLab 100
NEMO Designation {{{NEMO_Designation}}}
Lab Phone 215-898-9736
SOP Link QNF SOP

Description

The QNF Oxford Instruments PlasmaLab System 100 Plasma Enhanced Chemical Vapor Deposition (PECVD) tool is used to deposit a variety of thin-film materials at relatively modest temperatures on a variety of substrate materials. The tool utilizes an RF generator to deposit thin films at temperatures lower than traditional chemical vapor deposition systems. The tool operates between 150 and 350 C.


Applications
  • Silicon dioxide deposition
  • Silicon nitride deposition
  • Amorphous silicon deposition
Allowed material in PECVD System
  • Si, SixNy, SiO2, SOI, SiC, GaN
  • Al, Pt, Cr, W, Mo, Ti
  • Hard masks compatible with process temperature

List of materials NOT allowed in the chamber

Name symbol Melting Point [C]
Bismuth Bi 271
Cadmium Cd 321
Carbon C Subl.
Gallium Ga 30
Gold Au 1062
Indium In 157
Lead Pb 328
Lithium Li 179
Selenium Se 217
Sulfur S 115
Tellurium Te 452
Thallium Tl 302
Tin Sn 232
Zinc Zn 419

Process information

Standard process data - Table temperature fixed at 350 C

  • SiO2

Recipe parameters: optimized process parameters are in the report under "Protocols and Reports" section

Recipe name on the tool: Test-SiO2

Deposition rate: ~ 286 nm/min ± 2 nm/min


  • SiNx

Recipe parameters: optimized process parameters are in the report under "Protocols and Reports" section

Recipe name on the tool: Test-SiNx deposition

Deposition rate: ~ 45 nm/min ± 2 nm/min


  • a-Si

Recipe parameters: optimized process parameters are in the report under "Protocols and Reports" section

Recipe name on the tool: a-Si

Deposition rate: ~ 56 nm/min ± 3 nm/min

Special process data - adjustable table temperature

  • SiO2

Recipe parameters: optimized process parameters are in the report under "Protocols and Reports" section - table temperature at 200 C

Recipe name on the tool: Test-SiO2

Deposition rate: ~ 230 nm/min ± 2 nm/min