Difference between revisions of "Oxford PlasmaLab 100 PECVD"
Jump to navigation
Jump to search
| Line 17: | Line 17: | ||
== Description == | == Description == | ||
| − | The QNF | + | The QNF Oxford Instruments PlasmaLab System 100 Plasma Enhanced Chemical Vapor Deposition (PECVD) tool is used to deposit a variety of thin-film materials at relatively modest temperatures on a variety of substrate materials. The tool utilizes an RF generator to deposit thin films at temperatures lower than traditional chemical vapor deposition systems. |
| − | The QNF | + | The QNF Oxford Instruments PlasmaLab System 100 Plasma Enhanced Chemical Vapor Deposition |
===== Applications ===== | ===== Applications ===== | ||
Revision as of 09:42, 7 April 2022
| Tool Name | Oxford PlasmaLab 100 PECVD |
|---|---|
| Instrument Type | Deposition |
| Staff Manager | Sam Azadi |
| Lab Location | Bay 1 |
| Tool Manufacturer | Oxford |
| Tool Model | PlasmaLab 100 |
| NEMO Designation | {{{NEMO_Designation}}} |
| Nearest Phone | XXXXX |
| SOP Link | QNF SOP |
Description
The QNF Oxford Instruments PlasmaLab System 100 Plasma Enhanced Chemical Vapor Deposition (PECVD) tool is used to deposit a variety of thin-film materials at relatively modest temperatures on a variety of substrate materials. The tool utilizes an RF generator to deposit thin films at temperatures lower than traditional chemical vapor deposition systems.
The QNF Oxford Instruments PlasmaLab System 100 Plasma Enhanced Chemical Vapor Deposition
Applications
- Silicon dioxide deposition
- Silicon nitride deposition
- Amorphous silicon deposition
Allowed material in PECVD System
- Si, SixNy, SiO2, SOI
- Hard masks compatible with process temperature