Difference between revisions of "Lesker PVD75 E-beam Evaporator"
Jump to navigation
Jump to search
| Line 17: | Line 17: | ||
== Description == | == Description == | ||
| − | + | The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool. The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd via e-beam evaporation. | |
| Line 25: | Line 25: | ||
* Au | * Au | ||
* Pd | * Pd | ||
| − | |||
== Resources == | == Resources == | ||
Revision as of 10:26, 1 April 2022
| Tool Name | Lesker PVD75 E-Beam/Thermal Evaporator |
|---|---|
| Instrument Type | Deposition |
| Staff Manager | David Jones |
| Lab Location | Bay 2 |
| Tool Manufacturer | Kurt J. Lesker |
| Tool Model | PVD75 |
| NEMO Designation | {{{NEMO_Designation}}} |
| Nearest Phone | 8-9748 |
| SOP Link | SOP |
Description
The Kurt J. Lesker PVD75 E-beam Evaporator is an electron-beam (e-beam) evaporation tool. The tool is a fully automated system for depositing Ti, Cr, Au, and/or Pd via e-beam evaporation.
Films
- Ti
- Cr
- Au
- Pd