Revision as of 14:26, 29 April 2022
![]() |
|
Tool Name | Oxford Cobra ICP Etcher |
---|---|
Instrument Type | Etch |
Staff Manager | Sam Azadi |
Lab Location | Bay 2 |
Tool Manufacturer | Oxford Instruments |
Tool Model | Cobra PlasmaPro 100 |
NEMO Designation | {{{NEMO_Designation}}} |
Lab Phone | XXXXX |
SOP Link | SOP |
Description
Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures. The plasma created in the ICP tool is denser, which allows for a wider range of etching.
The tool is connected to the following gases: BCl3, Cl2, Ar, O2, SF6, CF4, and CHF3.
Applications
- Etch of Si
- Etch of SiO2
- Etch of SiNx