| Tool Name | Intlvac E-Beam Evaporator |
|---|---|
| Instrument Type | Physical vapor deposition |
| Staff Manager | David Barth |
| Lab Location | Bay 2 |
| Tool Manufacturer | Intlvac |
| Tool Model | Nanochrome |
| NEMO Designation | PVD-09 |
| Nearest Phone | 215-898-9748 |
| SOP Link | SOP |
Description
The tool
The IntlVac Electron Beam Evaporator has a base process chamber pressure in the low e-8 Torr range with substrate heating and ozone purging capabilities. Deposition rates are monitored by an automated magazine of 6MHz crystals. The tool can be used to process a single 4 inch wafer at a time or a selection of small chips/pieces.
Available materials
The tool contains the following materials:
- Al - Aluminum
- Ti - Titanium