Difference between revisions of "Total Internal Reflection Fluorescence AFM"
Jump to navigation
Jump to search
(Created page with "Category:Ambient AFM {{EquipmentInfo | name = TIRF-AFM | Tool_Name = TIRF-AFM | image = 300px | imagecaption = | Instrument_Type = AFM | Staff_Mana...") |
(update to NEMO) |
||
Line 11: | Line 11: | ||
| Tool_Manufacturer = Asylum / Nikon | | Tool_Manufacturer = Asylum / Nikon | ||
| Tool_Model = MFP-3D | | Tool_Model = MFP-3D | ||
− | | | + | | NEMO_Designation = TIRF-AFM |
| Lab_Phone = 8-9457 | | Lab_Phone = 8-9457 | ||
| SOP Link = [https://drive.google.com/file/d/1c9T_0DqiwEcC73Gxh6f4B_yrAiEq1GCT/view?usp=share_link SOP] | | SOP Link = [https://drive.google.com/file/d/1c9T_0DqiwEcC73Gxh6f4B_yrAiEq1GCT/view?usp=share_link SOP] |
Revision as of 14:26, 3 January 2024
![]() |
|
Tool Name | TIRF-AFM |
---|---|
Instrument Type | AFM |
Staff Manager | Matt Brukman |
Lab Location | Room 014 |
Tool Manufacturer | Asylum / Nikon |
Tool Model | MFP-3D |
NEMO Designation | TIRF-AFM |
Lab Phone | 8-9457 |
SOP Link | SOP |
Description
The TIRF-AFM is an atomic force microscope with an 80μm in-plane scan range and 13μm vertical scan range that can operate in ambient atmosphere or fluid environment installed on an inverted optical microscope with total internal reflection optics and three laser lines of illumination. Its dedicated prep lab has a CO2 incubator and bio safety cabinet for sample storage and plating.
Applications
- Fluorescent imaging of cells, proteins, tissues, and nanoparticles
- Nano-injection of drugs and dyes
- Topographic imaging in contact and tapping (AC) modes
- Stiffness, friction, and adhesion measurements
- Piezoelectric force microscopy
- Conductive AFM (ORCA mode)
- Scanning Kelvin Force (surface potential)
Accessories
- Micromanipulator + nanoinjector system
- Photometrics Prime 95B camera
- Nikon Eclipse Ti inverted optical microscope
- 633, 532, and 488 nm laser sources
- Dual-gain ORCA tipholder
- High-voltage PFM tipholder
- Polymer heater sample holder
- Humidity-sensing sample holder
- Fluid heater sample holder (shared with TIRF-AFM)