Difference between revisions of "ABM Mask Aligner"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
 
(One intermediate revision by the same user not shown)
Line 65: Line 65:
 
* [https://nemo.nano.upenn.edu/media/tool_documents/ma-03-abm-mask-aligner/MA-03_SOP_v01.pdf  SOP]
 
* [https://nemo.nano.upenn.edu/media/tool_documents/ma-03-abm-mask-aligner/MA-03_SOP_v01.pdf  SOP]
 
* [https://www.youtube.com/watch?v=cRzLljt0VLs Video - Standard procedure for previous model] *good overview, note slight differences*
 
* [https://www.youtube.com/watch?v=cRzLljt0VLs Video - Standard procedure for previous model] *good overview, note slight differences*
* [https://www.youtube.com/watch?v=Q1DvZBQgKhI&list=PLiihbHV9HgpX_9m5Khz2wn-XaxM5-yErU&index=16 Video - Alignment Marks ]
+
* [https://www.youtube.com/watch?v=Q1DvZBQgKhI&list=PLiihbHV9HgpX_9m5Khz2wn-XaxM5-yErU&index=16 Video - Alignment Marks ]  
 +
 
 +
===== [https://wiki.nano.upenn.edu/wiki/index.php?title=ABM3000HR_Mask_Aligner Calibration Instructions for Staff] =====

Latest revision as of 14:19, 15 May 2025


ABM Mask Aligner
Tool Name ABM Mask Aligner
Instrument Type Lithography
Staff Manager Ana Cohen
Lab Location Bay 6
Tool Manufacturer ABM
Tool Model
NEMO Designation MA-03
Lab Phone xxxxx
SOP Link SOP

Description

The ABM Mask Aligner is a manual and versatile mask aligner with top-side alignment and substrate capabilities from 100mm down to small pieces. Requires a 5" mask or 5" glass plate with film mask.

Applications

Tool is used primarily for SU8 exposure. It can also be used for aligning PDMS components for PDMS-to-PDMS bonding.

Exposure time = dose (mJ/cm^2) / intensity (mW/cm^2) Dose can be determined from the resist data sheet. See table below for intensities.

To obtain vertical sidewalls with a Cr glass mask, use the long pass filter (PL-360-LP) which eliminates UV emission below 350nm. Do not use with film masks. Inherent defects in film masks will be accentuated, resulting in worse results.

mW/cm^2 % of output
NO MASK ~10 100%
GLASS MASK ~9 87.5%
GLASS + FILM MASK ~7 68.5%
GLASS + LP FILTER ~5 47%
GLASS + FILM + LP FILTER ~4 37%

More information about Soft Lithography processing can be found under Process Resources