Difference between revisions of "Nanoscribe Photonic Professional GT"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(update tool owner)
 
(2 intermediate revisions by the same user not shown)
Line 8: Line 8:
 
| Instrument_Type = Lithography
 
| Instrument_Type = Lithography
 
| Staff_Manager = [[Ana Cohen | Ana Cohen]]
 
| Staff_Manager = [[Ana Cohen | Ana Cohen]]
| Lab_Location = Bay 2
+
| Lab_Location = Bay 6
 
| Tool_Manufacturer = Nanoscribe
 
| Tool_Manufacturer = Nanoscribe
 
| Tool_Model = Photonic Professional GT
 
| Tool_Model = Photonic Professional GT
| Iris_Designation = LW-02
+
| NEMO_Designation = LW-02
 
| Lab_Phone = XXXXX
 
| Lab_Phone = XXXXX
| SOP Link = [https://www.seas.upenn.edu/~nanosop/NanoScribe_3D_Printer.htm SOP]
+
| SOP Link = [https://nemo.nano.upenn.edu/media/tool_documents/lw-02-nanoscribe/LW-02_SOP_v01.pdf SOP]
 
}}
 
}}
  
Line 31: Line 31:
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
* [https://www.seas.upenn.edu/~nanosop/NanoScribe_3D_Printer.htm QNF SOP]
+
* [https://nemo.nano.upenn.edu/media/tool_documents/lw-02-nanoscribe/LW-02_SOP_v01.pdf QNF SOP]

Latest revision as of 18:22, 17 February 2025


Nanoscribe Photonic Professional GT
LW-02.jpeg
Tool Name Nanoscribe Photonic Professional GT
Instrument Type Lithography
Staff Manager Ana Cohen
Lab Location Bay 6
Tool Manufacturer Nanoscribe
Tool Model Photonic Professional GT
NEMO Designation LW-02
Lab Phone XXXXX
SOP Link SOP

Description

The Nanoscribe Photonic Professional is an easy-to-operate table-top laser lithography system that enables the fabrication of true three-dimensional nanostructures using commercially available photoresists. Designed for the fabrication of photonic crystal structures, the instrument is also ideal for, e.g., generating three-dimensional scaffolds for biology, micro- and nanofluidic circuitry.

Key Features
  • Laser power: 50-150 mW, Wavelength: 780 nm, Pulse ~100 fs, Repetition rate: 80 MHz
  • Available for Conventional 3D printing mode, Dip-in Liquid mode and air mode
  • 3D printing with lateral resolution ~ 200 nm, vertical resolution ~ 300 nm
  • High-precision Piezo scanning range: 300 x 300 x 300 μm3
  • Motorized XY-scanning range: 100 x 100 mm2