== Description ==
The EVG501 Wafer Bonding System is a highly flexible R&D system that can handle small substrate pieces up to 100 mm wafers. The new tool supports a variety of bonding processes, such as anodic, eutectic, diffusion, fusion, solder, and adhesive bonds, as well as other thermal processes, including oxide removal and high temperature bakes under a controlled atmosphere. The system also offers quick re-tooling with a conversion time of less than five minutes, making it ideal for universities and R&D as well as small-volume production applications.
+
The EVG510 Wafer Bonding System is a highly flexible R&D system that can handle small substrate pieces up to 100 mm wafers. The new tool supports a variety of bonding processes, such as anodic, eutectic, diffusion, fusion, solder, and adhesive bonds, as well as other thermal processes, including oxide removal and high temperature bakes under a controlled atmosphere. The system also offers quick re-tooling with a conversion time of less than five minutes, making it ideal for universities and R&D as well as small-volume production applications.
  
 
'''Specification'''
 
'''Specification'''

Revision as of 12:58, 9 February 2023


EVG 510 Wafer Bonder
BE-01.jpeg
Tool Name EVG 510 Wafer Bonder
Instrument Type Back End
Staff Manager Eric Johnston
Lab Location Bay 2
Tool Manufacturer EV Group
Tool Model 510
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone XXXXX
SOP Link SOP

Description

The EVG510 Wafer Bonding System is a highly flexible R&D system that can handle small substrate pieces up to 100 mm wafers. The new tool supports a variety of bonding processes, such as anodic, eutectic, diffusion, fusion, solder, and adhesive bonds, as well as other thermal processes, including oxide removal and high temperature bakes under a controlled atmosphere. The system also offers quick re-tooling with a conversion time of less than five minutes, making it ideal for universities and R&D as well as small-volume production applications.

Specification Maximum contact force: 10 kN Maximum temperature: 550 ºC Vacuum: ~0.1 mbar Power supply for anodic bonding: 0-2000 V and 50 mA


Applications
  • Anodic wafer bonding
  • Eutectic wafer bonding
  • Diffusion wafer bonding
  • Fusion wafer bonding
  • Adhesive wafer bonding


Resources

SOPs & Troubleshooting