Difference between revisions of "SCS PDS2010 Parylene Coater"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(Created page with "Category:Soft Lithography {{EquipmentInfo | name = SCS PDS2010 Parylene Coater | Tool_Name = SCS PDS2010 Parylene Coater | image = 300px | imagecapt...")
 
m
 
(12 intermediate revisions by 5 users not shown)
Line 1: Line 1:
[[Category:Soft Lithography]]
+
[[Category:Backend & Packaging]][[Category:Equipment]]
  
 
{{EquipmentInfo
 
{{EquipmentInfo
Line 6: Line 6:
 
| image = [[Image:PVD-07.jpeg|300px]]
 
| image = [[Image:PVD-07.jpeg|300px]]
 
| imagecaption =  
 
| imagecaption =  
| Instrument_Type = Soft Lithography
+
| Instrument_Type = Packaging
| Staff_Manager = Kyle Keenan  
+
| Staff_Manager = [[Kyle Keenan | Kyle Keenan]]
| Lab_Location = Bay 2
+
| Lab_Location = Singh 124
 
| Tool_Manufacturer = SCS
 
| Tool_Manufacturer = SCS
 
| Tool_Model = PDS2010
 
| Tool_Model = PDS2010
| Iris_Designation = PVD-07
+
| NEMO_Designation = PVD-07
 
| Lab_Phone = XXXXX
 
| Lab_Phone = XXXXX
 
| SOP Link = [https://www.seas.upenn.edu/~nanosop/Parylene_Coater_SOP.htm SOP]
 
| SOP Link = [https://www.seas.upenn.edu/~nanosop/Parylene_Coater_SOP.htm SOP]
Line 28: Line 28:
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
* [https://www.seas.upenn.edu/~nanosop/Parylene_Coater_SOP.htm QNF SOP]
+
* [https://upenn.box.com/s/yrchqkm3rc85g5oe6fd3pnv2xhu3cpt5 PVD-07 SOP]
 +
 
 +
 
 +
==== Process report ====
 +
* [https://repository.upenn.edu/scn_tooldata/45/ Characterization and Optimization of Parylene-C deposition process using SCS Parylene coater]

Latest revision as of 12:39, 28 July 2025


SCS PDS2010 Parylene Coater
PVD-07.jpeg
Tool Name SCS PDS2010 Parylene Coater
Instrument Type Packaging
Staff Manager Kyle Keenan
Lab Location Singh 124
Tool Manufacturer SCS
Tool Model PDS2010
NEMO Designation PVD-07
Nearest Phone XXXXX
SOP Link SOP

Description

The SCS Labcoter 2 (PDS 2010) vacuum deposition system is specifically designed to bring Parylene technology to the laboratory. Its size and portability make it the ideal choice for universities and research institutions looking to develop and design with Parylene conformal coatings.

As a high quality, compact coating unit, the PDS 2010 is well suited for a range of applications, including circuit boards, sensors, wafers, medical devices and elastomeric components for research, development and repair.

Applications
  • Conformal parylene coating of substrates


Resources

SOPs & Troubleshooting


Process report