Difference between revisions of "Filmetrics F40"
Jump to navigation
Jump to search
(update tool owner, update to NEMO) |
m |
||
| (One intermediate revision by the same user not shown) | |||
| Line 1: | Line 1: | ||
| − | [[Category:Metrology]] | + | [[Category:Metrology]][[Category:Equipment]] |
{{EquipmentInfo | {{EquipmentInfo | ||
| Line 8: | Line 8: | ||
| Instrument_Type = Metrology | | Instrument_Type = Metrology | ||
| Staff_Manager = [[David Barth | David Barth]] | | Staff_Manager = [[David Barth | David Barth]] | ||
| − | | Lab_Location = | + | | Lab_Location = Cleanroom Corridor |
| Tool_Manufacturer = Filmetrics | | Tool_Manufacturer = Filmetrics | ||
| Tool_Model = F40 | | Tool_Model = F40 | ||
Latest revision as of 12:33, 28 July 2025
| Tool Name | Filmetrics F40 |
|---|---|
| Instrument Type | Metrology |
| Staff Manager | David Barth |
| Lab Location | Cleanroom Corridor |
| Tool Manufacturer | Filmetrics |
| Tool Model | F40 |
| NEMO Designation | MET-04 |
| Nearest Phone | XXXXX |
| SOP Link | SOP |
Description
The Filmetrics F40 is a microscope-mounted thin-film measurement system, allowing you to non-destructively measure thin-film thicknesses in small (patterned) areas on your sample. The Filmetrics software then performs curve-fitting to determine the thickness and/or refractive index of the measured films.
Applications
- Thin-film thickness optical measurements