Difference between revisions of "Nanoscribe Photonic Professional GT"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
m (Protected "Nanoscribe Photonic Professional GT" ([Edit=Allow only administrators] (indefinite) [Move=Allow only administrators] (indefinite)) [cascading])
 
(4 intermediate revisions by 2 users not shown)
Line 7: Line 7:
 
| imagecaption =  
 
| imagecaption =  
 
| Instrument_Type = Lithography
 
| Instrument_Type = Lithography
| Staff_Manager = David Jones
+
| Staff_Manager = [[Ana Cohen | Ana Cohen]]
| Lab_Location = Bay 2
+
| Lab_Location = Bay 6
 
| Tool_Manufacturer = Nanoscribe
 
| Tool_Manufacturer = Nanoscribe
 
| Tool_Model = Photonic Professional GT
 
| Tool_Model = Photonic Professional GT
| Iris_Designation = LW-02
+
| NEMO_Designation = LW-02
 
| Lab_Phone = XXXXX
 
| Lab_Phone = XXXXX
| SOP Link = [https://www.seas.upenn.edu/~nanosop/NanoScribe_3D_Printer.htm SOP]
+
| SOP Link = [https://nemo.nano.upenn.edu/media/tool_documents/lw-02-nanoscribe/LW-02_SOP_v01.pdf SOP]
 
}}
 
}}
  
Line 31: Line 31:
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
* [https://www.seas.upenn.edu/~nanosop/NanoScribe_3D_Printer.htm QNF SOP]
+
* [https://nemo.nano.upenn.edu/media/tool_documents/lw-02-nanoscribe/LW-02_SOP_v01.pdf QNF SOP]

Latest revision as of 18:22, 17 February 2025


Nanoscribe Photonic Professional GT
LW-02.jpeg
Tool Name Nanoscribe Photonic Professional GT
Instrument Type Lithography
Staff Manager Ana Cohen
Lab Location Bay 6
Tool Manufacturer Nanoscribe
Tool Model Photonic Professional GT
NEMO Designation LW-02
Lab Phone XXXXX
SOP Link SOP

Description

The Nanoscribe Photonic Professional is an easy-to-operate table-top laser lithography system that enables the fabrication of true three-dimensional nanostructures using commercially available photoresists. Designed for the fabrication of photonic crystal structures, the instrument is also ideal for, e.g., generating three-dimensional scaffolds for biology, micro- and nanofluidic circuitry.

Key Features
  • Laser power: 50-150 mW, Wavelength: 780 nm, Pulse ~100 fs, Repetition rate: 80 MHz
  • Available for Conventional 3D printing mode, Dip-in Liquid mode and air mode
  • 3D printing with lateral resolution ~ 200 nm, vertical resolution ~ 300 nm
  • High-precision Piezo scanning range: 300 x 300 x 300 μm3
  • Motorized XY-scanning range: 100 x 100 mm2