Difference between revisions of "KLA Tencor P7 2D profilometer"
Jump to navigation
Jump to search
(update tool owner, update to NEMO) |
|||
| Line 8: | Line 8: | ||
| Instrument_Type = Metrology | | Instrument_Type = Metrology | ||
| Staff_Manager = [[David Barth | David Barth]] | | Staff_Manager = [[David Barth | David Barth]] | ||
| − | | Lab_Location = | + | | Lab_Location = Cleanroom Corridor |
| Tool_Manufacturer = KLA | | Tool_Manufacturer = KLA | ||
| Tool_Model = P7 | | Tool_Model = P7 | ||
Revision as of 10:44, 28 June 2024
| Tool Name | KLA Tencor P7 2D profilometer |
|---|---|
| Instrument Type | Metrology |
| Staff Manager | David Barth |
| Lab Location | Cleanroom Corridor |
| Tool Manufacturer | KLA |
| Tool Model | P7 |
| NEMO Designation | MET-01 |
| Nearest Phone | XXXXX |
| SOP Link | SOP |
Description
The KLA-Tencor P7 Profiler is a highly sensitive surface profiler that measures step height, roughness, and waviness on sample surfaces. The KLA-Tencor Profiler systems use stylus-based scanning to achieve high resolution.
Applications
- Film step height measurements
- Photo resist thickness
- Etched trench depth
- Materials characterization for surface roughness and waviness