KLA Tencor P7 2D&3D/stress profilometer
MET-02.jpeg
Tool Name KLA Tencor P7 2D&3D/stress profilometer
Instrument Type Metrology
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer KLA
Tool Model P7
NEMO Designation {{{NEMO_Designation}}}
Lab Phone XXXXX
SOP Link SOP

Description

The KLA-Tencor P7 Profiler is a highly sensitive surface profiler that measures step height, roughness, and waviness on sample surfaces. The KLA-Tencor Profiler systems use stylus-based scanning to achieve high resolution.

Applications
  • Film step height measurements
  • Photo resist thickness
  • Etched trench depth
  • Materials characterization for surface roughness and waviness
  • Wafer bow / stress measurements