Jupiter II RIE Plasma Etcher
Revision as of 14:44, 29 March 2022 by Trevinoj (talk | contribs) (Created page with "Category:Etch {{EquipmentInfo | name = Jupiter II RIE Plasma Etcher | Tool_Name = Jupiter II RIE Plasma Etcher | image = 300px | imagecaption = | In...")
Tool Name | Jupiter II RIE Plasma Etcher |
---|---|
Instrument Type | Etch |
Staff Manager | Sam Azadi |
Lab Location | Bay 2 |
Tool Manufacturer | March |
Tool Model | Jupiter II |
NEMO Designation | {{{NEMO_Designation}}} |
Lab Phone | XXXXX |
SOP Link | SOP |
Description
The March Jupiter II is a reactive ion etcher configured with O2 gas. The system is typically used as a plasma asher/cleaner.
Applications
- Removal of photoresist
- Removal of organic materials