Difference between revisions of "Fiji G2 ALD"
Jump to navigation
Jump to search
(Created page with "Category:Deposition {{EquipmentInfo | name = Veeco Fiji G2 | Tool_Name = Veeco Figi G2 | image = 300px | imagecaption = | Instrument_Type = Deposit...") |
|||
(2 intermediate revisions by the same user not shown) | |||
Line 3: | Line 3: | ||
{{EquipmentInfo | {{EquipmentInfo | ||
| name = Veeco Fiji G2 | | name = Veeco Fiji G2 | ||
− | | Tool_Name = Veeco | + | | Tool_Name = Veeco Fiji G2 |
| image = [[Image:ALD-03.jpeg|300px]] | | image = [[Image:ALD-03.jpeg|300px]] | ||
| imagecaption = | | imagecaption = | ||
Line 17: | Line 17: | ||
== Description == | == Description == | ||
− | Fiji is a plasma and thermal ALD equipped with high-speed pneumatic pulse valves to enable our unique Exposure Mode for thin film deposition on Ultra High Aspect Ratio substrates. This proven precision thin film coating methodology can be used to deposit conformal, uniform films on substrates with aspect ratios of greater than > 2000:1. | + | Fiji is a plasma and thermal ALD equipped with high-speed pneumatic pulse valves to enable our unique Exposure Mode for thin film deposition on Ultra High Aspect Ratio substrates. This proven precision thin film coating methodology can be used to deposit conformal, uniform films on substrates with aspect ratios of greater than > 2000:1. Fiji is capable of holding substrates of different sizes up to 200mm. The Fiji thin film deposition system is equipped with TMA, DEZ, and water. |
===== Films ===== | ===== Films ===== | ||
* Al2O3 | * Al2O3 | ||
* ZnO | * ZnO |
Latest revision as of 13:47, 20 March 2024
Tool Name | Veeco Fiji G2 |
---|---|
Instrument Type | Deposition |
Staff Manager | Sam Azadi |
Lab Location | Bay 2 |
Tool Manufacturer | Veeco |
Tool Model | Fiji G2 |
NEMO Designation | ALD-02 |
Lab Phone | 215-898-9736 |
SOP Link | SOP |
Description
Fiji is a plasma and thermal ALD equipped with high-speed pneumatic pulse valves to enable our unique Exposure Mode for thin film deposition on Ultra High Aspect Ratio substrates. This proven precision thin film coating methodology can be used to deposit conformal, uniform films on substrates with aspect ratios of greater than > 2000:1. Fiji is capable of holding substrates of different sizes up to 200mm. The Fiji thin film deposition system is equipped with TMA, DEZ, and water.
Films
- Al2O3
- ZnO