Resists at QNF
Jump to navigation
Jump to search
The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed.
QNF Supplied Standard Photoresists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
S1805 | + | General | KL5305 | Datasheet |
S1813 | + | General | KL5315 | Datasheet |
S1818 | + | General | Datasheet | |
SPR 220-3 | + | Etch | KPRO-3, KL6003, AZ3330F | Datasheet |
SPR 220-4.5 | + | Etch | KPRO-3, KL6003, AZ3330F | Datasheet |
SPR 220-7 | + | Etch | AZ 12XT, AZ P4620 | Datasheet |
AZ 3330F | + | General, Metal RIE, Plating | SPR 220-3, SPR 220-4.5, K-PRO 3, KL6003 | Datasheet |
NR7-3000P | - | Etch, General | Datasheet | |
APOL-LO 3202 | - | Liftoff | Datasheet | |
IP-Dip | - | Nanoscribe | ||
HARE SQ 2 | - | Epoxy | SU-8 2005 | Datasheet |
HARE SQ 50 | - | Epoxy | SU-8 2050 | Datasheet |
Stockroom Photoresists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
SU-8 2005 | - | Epoxy | HARE SQ 2 | Datasheet |
SU-8 2050 | - | Epoxy | HARE SQ 50 | Datasheet |
SU-8 2100 | - | Epoxy | HARE SQ 50 | Datasheet |
SU-8 3050 | - | Epoxy | HARE SQ 50 | Datasheet |
Standard e-beam Resists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
495 PMMA A8 | + | Lower Resolution | Datasheet | |
495 PMMA A4 | + | Lower Resolution | Datasheet | |
495 PMMA A2 | + | Lower Resolution | Datasheet | |
950 PMMA A4 | + | High Resolution | Datasheet | |
950 PMMA A2 | + | High Resolution | 1000 HARP 0.1 | Datasheet |
1000 HARP 1.3 | + | High Resolution | Datasheet | |
1000 HARP 0.1 | + | High Resolution | 950 PMMA A2 | Datasheet |
Stockroom e-beam Resists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
ZEP 520A | + | Thicker formulation | Datasheet | |
ZEP 520A-7 | + | Thinner formulation | Datasheet | |
H-SiQ 6% | - | HSQ Equivalent | Datasheet |